@AshokKushwaha-zv1cg
@AshokKushwaha-zv1cg 8 күн бұрын
Sir please make a video of presso film in field joint coating
@sayyednaveedislam6661
@sayyednaveedislam6661 29 күн бұрын
Great work sir
@sebaestschn1
@sebaestschn1 Ай бұрын
What is the norm for this test? Usually this test is carried out at 23°C, but OK, infield can deviate. Moreover, usually, you pull max possible force to figure out the peel strength. The resolution is not good, but the applied force seems to be pretty low. This product can handle way more 😉
@nagendrachhetri4965
@nagendrachhetri4965 Ай бұрын
Very nice 👍 work
@nagendrachhetri4965
@nagendrachhetri4965 Ай бұрын
Good 👍
@IsmailTaufek
@IsmailTaufek Ай бұрын
Lol
@sunilgupta573
@sunilgupta573 Ай бұрын
HTLP 80 normal sleev & Direx sleev thickness ??? please tell me Sir
@sunilgupta573
@sunilgupta573 Ай бұрын
Dear sir, direx sleev and normal sleev melting point??
@mrlonely265
@mrlonely265 Ай бұрын
WHAT IS THE DIGITAL INSTRUMENT NAME
@tilakrajsingh7173
@tilakrajsingh7173 2 ай бұрын
Good work sir 👍
@shasegirimatta3136
@shasegirimatta3136 2 ай бұрын
Nice Bava Garu 🎉
@nasirmalik5103
@nasirmalik5103 2 ай бұрын
Yes Sir quality is first of all... I'm QC Inspector 16 years experience.
@nasirmalik5103
@nasirmalik5103 2 ай бұрын
I have all information about 3 layer and FBE Internal and External coating... Al Qahtani Pipe Coating Industries...
@tilakrajsingh7173
@tilakrajsingh7173 2 ай бұрын
Good work sir 🙏
@kapildevpandey224
@kapildevpandey224 2 ай бұрын
Very good information 👍👍👍sir
@jayoza3005
@jayoza3005 2 ай бұрын
In case if you purchase this sleeve you need to purchase primer😊
@hassanzaib2245
@hassanzaib2245 2 ай бұрын
v informative
@johnzhang9537
@johnzhang9537 2 ай бұрын
You also try TSD80 Heat shrink sleeve?
@qaiseraziz6773
@qaiseraziz6773 3 ай бұрын
👌
@عليخلفطاهر-ل2ج
@عليخلفطاهر-ل2ج 3 ай бұрын
Thanks 🙏
@sufyanakhtar8027
@sufyanakhtar8027 3 ай бұрын
Sir I have your contact number pls.
@thekop1225
@thekop1225 4 ай бұрын
Mr.Narongsak 's Worley
@FirozKhan-vf2jh
@FirozKhan-vf2jh 4 ай бұрын
Sir send me number
@AMRITALADHA
@AMRITALADHA 4 ай бұрын
SIR CAN I GET YOUR EMAIL ID, I HAVE FEW QUERIES REGARDING COLD APPLIED PE TAPES
@kesavakumarthecompletefami9610
@kesavakumarthecompletefami9610 2 ай бұрын
@Abdullatif-dj2of
@Abdullatif-dj2of 5 ай бұрын
Sir I went to all notes for how to coating process
@Abdullatif-dj2of
@Abdullatif-dj2of 5 ай бұрын
Very useful video
@Abdullatif-dj2of
@Abdullatif-dj2of 5 ай бұрын
Think you sir
@mkommkom9542
@mkommkom9542 5 ай бұрын
what professional qualification do you have or what position?
@kesavakumarthecompletefami9610
@kesavakumarthecompletefami9610 2 ай бұрын
I am a technical manager at Seal for life.
@Ravindrakumar-et1nm
@Ravindrakumar-et1nm 5 ай бұрын
Shir coating me kaun kaun sa stumeant name check karane wala stumeant
@claytonbelocura5169
@claytonbelocura5169 6 ай бұрын
So 180 microns deduct instead of 50?if so how to justify to consultant?
@kesavakumarthecompletefami9610
@kesavakumarthecompletefami9610 6 ай бұрын
Deduct 50 microns of film thickness from the final reading.
@claytonbelocura5169
@claytonbelocura5169 6 ай бұрын
What? Any English subtitle pls
@badebhai1642
@badebhai1642 6 ай бұрын
Good
@sudhir.kudtarkar13
@sudhir.kudtarkar13 6 ай бұрын
Very nice information thanks
@drstanleyrodriguez6675
@drstanleyrodriguez6675 6 ай бұрын
DEAR SIR,I HAVE DONE MY BTECH IN METALLURGICAL ENGINEERING AND DID JOB FOR 2 YEARS,QUIT JOB FOR HEALTH REASONS,NOW PLANNING AGAIN TO DO JOB,I HEARD ABOUT PAINTING INSPECTOR COURSE OF BGAS AND NACE,WHATS THE FUTURE AND SHOULD I DO IT???/NEEED YOUR ADVICE
@SunilMahi-ky5eo
@SunilMahi-ky5eo 6 ай бұрын
Ok sir
@Subramanian2020
@Subramanian2020 6 ай бұрын
Trilling experience your patience is appreciative,God will be always with you sir
@liquidfootball8833
@liquidfootball8833 7 ай бұрын
Frame should be pneumatic powered. Inadequate PPE for FBE application. Poor overlap preparation. PIH perform better and that is an insult of the highest regard.
@ravichaudhary3363
@ravichaudhary3363 7 ай бұрын
Great sir ji
@SunilMahi-ky5eo
@SunilMahi-ky5eo 7 ай бұрын
Coating Internal pending ka video daliye sir
@jaikeebarnwal1475
@jaikeebarnwal1475 7 ай бұрын
Hello sir costing ka meteriyal ka kta kya nam hi sir iska bhi ek vidio banaiye
@EG-zs7ut
@EG-zs7ut 7 ай бұрын
The thickness is not consistent !!!!!
@Raj-ko2gl
@Raj-ko2gl 8 ай бұрын
Not clear properly
@FirozKhan-vf2jh
@FirozKhan-vf2jh 9 ай бұрын
Sir apna number send kijiye
@kesavakumarthecompletefami9610
@kesavakumarthecompletefami9610 9 ай бұрын
As per ASTM D1000.
@zhanbolat5654
@zhanbolat5654 9 ай бұрын
Sir, please can you tell us, according to which standard this peel test has been conducted ? (60 seconds up to 100mm applying 2.5 kg)
@TRADIVEST.....5178
@TRADIVEST.....5178 9 ай бұрын
Sir agar 5 kag me crass kar deta to aur 5 kg pr adhesion nikal ke chala aata to failure hai???
@TRADIVEST.....5178
@TRADIVEST.....5178 9 ай бұрын
Sir your contact is very informative please don't stop the share humble request
@jayoza3005
@jayoza3005 10 ай бұрын
Where can i purchase perp 80 material?
@kesavakumarthecompletefami9610
@kesavakumarthecompletefami9610 9 ай бұрын
You can send a mail to [email protected]
@frankhurt6083
@frankhurt6083 10 ай бұрын
I don't understand what you are saying
@kesavakumarthecompletefami9610
@kesavakumarthecompletefami9610 9 ай бұрын
The complete FJC process Explained in local language ( Hindi).
@ghmustafa4121
@ghmustafa4121 10 ай бұрын
After coating HDD section, minimum time to pull pls reply.
@kesavakumarthecompletefami9610
@kesavakumarthecompletefami9610 9 ай бұрын
As per the specification 24 hours.