A much neglected but important topic. Your methodology is sound, intuitive, logical and illustrative. Thank you.
@littlepacificstudios Жыл бұрын
What do you think about Delrin plastic about holding after weeks under load?
@genegreiner77663 жыл бұрын
Thank you for creating content that is innovative instead of just copying what others have done. You are contributing to the knowledge of the printing community. I just began supporting you on Patreon. Thanks!
@MyTechFun3 жыл бұрын
Thank you Gene, I appreciate that! More similar test are comming.. with different materials (PC, PA, ABS+ etc)
@sandrolauer3503 жыл бұрын
Excellent! Creeping is too often overseen in 3d-print material tests but has so much impact when dealing with plastics. Thank you! Btw: in my experience the gap between PETG and ABS is truly noticable in real life parts, therefore I moved to ABS. But might depend on the brand.
@WhenDoesTheVideoActuallyStart2 жыл бұрын
The Voron community only uses ABS because of it's creep resistance
@alejandroperez53682 жыл бұрын
@@WhenDoesTheVideoActuallyStart Prusa printers use PETG. So, you tell me.
@WhenDoesTheVideoActuallyStart2 жыл бұрын
@@alejandroperez5368 And? ABS is still better at creep resistance than PETG. Prusa uses PETG it's because they had the freedom to design a printer with parts that only required certain specific properties, and had the freedom to design both the models and the polymer blend to meet those needs. Besides, they're mostly there for aligning parts, almost none of them are load-bearing. The Voron team doesn't sell printers, they can't hire factories to produce specific metal parts for their printers or fabricate their own filament blends, they're just a grouplet of hobbyists designing printers from parts that are available off-the-shelf, so they have far more limitations. The Voron team had to design their printers around the minimum properties of common off-the-shelf filament blends and chose ABS, despite the eternal nagging by new people about the possibility of using polyamide or PETG - their printers simply won't perform well with those.
@Chad.The.Flornadian3 жыл бұрын
Aside from the actual content itself, which is very thorough and informative, I wanted to commend you for the way you presented it. Your video editing skills have greatly improved. I enjoy your use of time lapse, speeding up, and splicing shots together.
@christopherrumford3 жыл бұрын
Fantastic video, I really appreciate the scientific methods for testing of the material properties. A DTI gauge jig for all printed peices would be a massive time saver for future videos. Keep doing what your doing,you've planned out and documented your finding like a pro. You deserve more viewers to the channel,keep it scientific and the nerds will keep on subscribing. The torque test was very useful,and the reletively low deformation temperature for PLA was eye opening. Very much looking forward to the ABS results in your upcoming video. Thanks for taking the time to experiment and document your findings for us.
@kachler672 жыл бұрын
One theory about the immense creep of the Nylon samples: as we all know, it takes up a lot of moisture (up to 10% in weight), which it does after printing as well. I recently stumbled upon a statement of a material science student, who investigated the mechanical properties after leaving the parts out in the open. He stated, that the elastic modulus was almost half compared to freshly printed ones. So the creep of Nylon could actually also be down to moisturizing, maybe it would be interesting to see how „old“ parts would perform the same test
@inmyimage10812 жыл бұрын
I’m new to 3d printing and trying to decide what my go to filaments are going to be for differentiate cases. I’ve watched a couple of your videos in addition to those from other creators now and yours are far the best thought out, scientific and controlled. Subscribed and looking forward to new videos and watching your testing methodology refine over time.
@oasntet2 жыл бұрын
The compression creep tests are fascinating. I had a functional print with a live hinge compressed around a pipe, and over time the PLA it was printed in migrated away from the bolt until it became impossible to tighten it anymore. I was hoping to find PETG or ASA had less creep under compression, but evidently not. I guess the best that can be done is to print the compressed area at 100% infill and use the largest washer I can fit in that area. Or carve it out of wood... In any case, your data and collection methods are really handy, thanks for the data!
@clborrello3 жыл бұрын
Great video. Please continue to do these creep tests with other materials! There are so many interesting filaments out there and hardly any information on creep.
@WorldPowerLabs Жыл бұрын
Outstanding work! Clever, thorough tests. There are many channels with discussions about the physical properties of different filament types, but few conduct meaningful tests.
@danne77sthlm3 жыл бұрын
These type of tests is always good, especially if you like me like to print functional parts and build things like rc cars etc, so I like this
@tanvach2 жыл бұрын
Amazing, thank you for testing this. Creep is something I've noticed for tight tolerance parts loosening over time.
@BrandonWhipp3 жыл бұрын
Very much anticipating the ABS test.
@epleace2 жыл бұрын
Thank you very much, very helpful and careful tests. I am printing a spring for a battery holder. The PLA spring deformed under the small tension of holding the battery. Based on your test I'll try PETG.
@suivzmoi2 жыл бұрын
a valuable resource for the 3d printing community for years to come
@grantmelocik17033 жыл бұрын
Thank you you Igor for an excellent and super helpful test. I have also found ASA to be most useful for outdoor parts that see heat but always wanted to see actual tests like yours.
@brappineau41612 жыл бұрын
Great job, one of the best videos I've seen so far. I would love to see the weight test outdoors on a hot summer day
@MyTechFun2 жыл бұрын
It would be similar as in enclosure. And maybe you will find this one interesting too: not outside, but in car: kzbin.info/www/bejne/h5WkfJeVjsemoKs
@UniformWhiskyEcho2 жыл бұрын
I really like these additions to your tests. I'm all for tests that are more relatable to real world scenarios rather than ISO lab tests. For the torque test maybe you can include the total amount (added up) of degrees turned after 6 days. This would relate to "tightened additional 2 full turns".
@marcokunz97153 жыл бұрын
Would like to see: Nonoilen, Carbon fiber blends, "low odor" ABS (eg Novamaker), PC blends printable below 250 C (eg PC-PETG blend like zhoupu brand)
@Adlore3 жыл бұрын
I was thinking about this when designing a part today. Keen to see the results
@qozia1370 Жыл бұрын
Wow! This video is a treasure of information! Much respect and love.
@qozia1370 Жыл бұрын
Subscribed!
@The_Privateer3 жыл бұрын
Awesome testing! I'd be interested to see how polycarbonate would do.
@MyTechFun3 жыл бұрын
I just got some ePC, ePA, ABS+ from eSun, so there will be a polycarbonate test in very near future (not only creep test)
@Londubh3 жыл бұрын
This is awesome. Might I recommend a slightly different "screw" test? Instead of testing how much you can rotate the screws at a given torque, a more in-machine relevant test might be to test the torque required to break the nuts free. Procedure: Tighten nuts to a specified torque (using your high-repeatability click wrench), then check the maximum torque required to "break free" using your digital one. If the material softens, there won't be as much pressure against the threads, and it should have a lower "break free" torque.
@MyTechFun3 жыл бұрын
Hm, great point, if I understand correctly. Instead additional tightening the screw, more important is the torque for loose the screw. That also a realistic case too. Perfect would be if I could measure the pressure between 3D printed object and the nut or washer for example. Imagine you use screw to join two parts, you want that pressure between two parts to be constant and strong. Now, that's hard to measure. What I can easily measure, is additional twisting the screw (which is in linear corelation with that pressure), as you can see in video. Maybe at the end of the test, I could measure the unscrewing torque too.
@joshua432143 жыл бұрын
This would be very difficult to get repeatable results since a great deal will depend on layer adhesion. You are describing a shearing test in essence.
@parkerbradshaw41222 жыл бұрын
@@MyTechFun the most relevant statistic for screws in plastic is how the clamping load decreases over time, this is usually what's speced out in injection molding plastics tech sheets. However this is sometimes hard to measure, requiring a load cell/strain gauge
@OsaderLP2 жыл бұрын
Wow, that's really professional! Your results correlate with the general opinion the engineers have at my work. PA (or Nylon) has wildly different creep depending on ingredients, if everything fails, add glass fiber :) Thanks for going through all that work, analyzing and documenting! This should have more views.
@William3DP2 жыл бұрын
You not only have an excellent channel with excellent videos, but you also have a new subscriber.
@jabberwocktechnologies Жыл бұрын
Thanks for the info! The screw test is extremely relevant since it's very similar to the kinds of loads some printed parts face when they're actually in use. I'm curious about whether annealing would help the nylon (or PLA) too.
@mario_nuevo3 жыл бұрын
I'm missing PACF and PCCF filaments. Those are commonly used in printers parts, and after some people complaining about PACF creeping, my choice could be PCCF.
@MyTechFun3 жыл бұрын
I got some filaments from eSun for testing. ABS+, ePA and ePC (not CF), there will be a comparison video too. But carbon fiber tests will be included in near future. Only waiting for some hardened nozzles to arrive.
@5bitesrods3 жыл бұрын
I also am very interested in the carbon fiber blend filaments. I look forward to the results.
@fuall69933 жыл бұрын
Good information, I've only printed with PLA & PLA+ we use them for 3D printing guns and parts
@davidnemeth20953 жыл бұрын
I really like your experiment designs.
@krakatoa19872 жыл бұрын
Excellent job, very informative and entertaining to see, thank you and will be waiting for the ABS and other materials test. subscribed!
@SianaGearz3 жыл бұрын
This is something i needed! I would like to add untreated PLA vs annealed PLA comparison to the test, i wonder if annealed PLA will perform better. Also a material that often gets neglected in tests is HIPS. It is very inexpensive! It's supposed to shrink less than ABS in printing, and similar to ASA, and be more rigid and less smelly than ABS, though smell potential exists, and high shrinkage potential exists too. I think i would like to see more of it. I think there can be a massive difference between brands, as opposed to ASA or PETG or most non-silk PLAs, which is unfortunate. I do like the C-shape test, in the absence of other tests, so if i had to choose just one test out of 3, i would make a decision based on it alone, and it's fine to me as-it-is; but i think screw test is interesting too, it looks like it will provide interesting and distinctive results eventually. I also actually liked all the tests though. Maybe if you use a piece of double sided tape to secure the nut, nylon can survive the 2-point test too, well enough to make a measurement, with enough room for it to bend down. But it also looks like the most fragile of the tests, with potentially needing a different thickness of the sample depending on modulus to be comparable. 45°C is an excellent choice for a hot box, as it's more or less representative for example also of use inside a car or inside a computer. Normally say you can expect the air in the computer chassis to become 40°C under load and SSD or hard disk can also reach 45°C. Currently i have a 3D printed SSD retainer in my PC and will probably have a 3D printed CPU cooler mount in my next PC. Ideally i won't have a 3D printed backplate but we'll see. I recall Stefan (CNC Kitchen) did have a 3D printed CPU cooler retainer and it failed on him, and it was i think CF Nylon? In hindsight, not surprising. He also experienced his Voron fail in exactly the same manner, with material creep under mild heat! I actually don't terribly mind PLA being used for part cooling fan assemblies and such, because they aren't really load bearing, and also can survive some permanent deformation. But i do think PLA is less ideal.
@MyTechFun3 жыл бұрын
Thanks for your detailed comment. Yes, any kind of nylon (CF nylon) have this creep problem, it is good in impact tests for example. 2 point bending test I will replace with 3 point, only I have to solve the problem of accurate reading (with dial indicator, more accurate). And on my list is testing of annealed PLA vs PLA (and vs Nonoilen filament, because it is PLA type but heat resistant up to 110°C without annealing, tested earlier). For ABS testing for voron parts probably I have to go higher, up to 50C (accorting to response to my question in Voron group) and for longer time, not only 2 hrs. Mayabe 4-6h.
@jullit312 жыл бұрын
@@MyTechFun Thanks for the great video! I'd also be very interested in results for annealed PLA. Nonoilen seems to be similar to extrudr GreenTEC Pro, maybe that would also be a good candidate for testing...
@ZappyOh3 жыл бұрын
Perfect topic for some of my current projects ... thx :)
@davidosterberg2 жыл бұрын
Would be interesting to know the stress in the material in the tests. Is there a critical stress below which there is negligible creep?
@user-xb5zu6zu7j3 жыл бұрын
I was waiting for a video just like this! Thanks
@ovalwingnut3 жыл бұрын
Very interesting, Egor.. Thank you. I don't have a 3D printer but I DO have a curious mind. That's all that was really needed to enjoy your vid. GR8T post editing by the way. That was a chor in itself. Cheers from So.Ca.USA, 3rd House On the Right.
@LeonMatthews2 жыл бұрын
Fantastic methodology. I really respect your attention to detail. I'd only suggest that your graphs be modified to show just the deformation for readability, ie. for test one subtract 12mm. Very informative.
@MyTechFun2 жыл бұрын
Yes, I am using that method now in newest videos (deformation, difference between two days)
@maximilian.arnold3 жыл бұрын
I really enjoy your investigations! Nicely done.
@davidg58983 жыл бұрын
I thought the screw test was useful and would happy to see if you can develop it a little more to get more meaningful numbers from it. Maybe have the screws hold 2 pieces together with a pressure sensor in between (Arduino/Raspberry Pi pressure pads are pretty cheap). That way you can test if the clamping force is actually weakening over time, if the additional twisting to the same torque is actually increasing pressure or not, etc. Something else I'd like really like to see is some testing in the cold. I like the higher temperature tests you do. No one seems to test for the cold, even though many people print things that are meant for outdoors or to be kept in a car. How do prints with different filaments change in strength, flexibility, and brittleness at or below 0°C?
@MyTechFun3 жыл бұрын
I got your point, and you are right. I have some pressure sensors, BUT it is not so easy to use them, I need two equal or one with hole. Place it simmetric etc. That's why I measure this torque, because it is in linear correlation with that force between two parts. About cold test, great idea, definitely I will test it, winter is comming, I hope I will have -10°C outside :-) And I am curious not only for creep test, but also tensile, layer adhesion etc.
@stefanguiton3 жыл бұрын
Excellent videos as always Igor!
@rondlh20 Жыл бұрын
Amazing tests again, great job!
@FrankLauerSignalSpirit Жыл бұрын
Nice Video. I would suggest to normalize the results to get a % value (eg. Platic defimation/lenth). I have done similar measurements with another geometry. In my measurement PLA and PETG performes quite similar (20°C). But annihling the parts used to have an extrem impact on the creeping. It more than halves the creeping (also on PETG). The effect of the annihling was much much bigger than the difference between the materials. With Extrudr NX2 I also have found a PLA, wich dos not deform so much during the annihling.
@thiagosannafreiresilva43663 жыл бұрын
Great test! I would like to see annealed PLA as well, together with Colorfabb XT or HT and Taulman Alloy 910.
@Exstaz3 жыл бұрын
Great test. Just a question about the nylon. It looks like it was not dried before use, looks like you can see that it has bin bubbling when extrudes. You also did not mention if the nylon have had time to equalize with the humidity. Freshly printed nylon get softer over time cause it absorbs moisture.
@MyTechFun3 жыл бұрын
Nylon was dried, but probably not enough. 4h at 70C (it is recommended 12h at 70C, but I thought that it stay dry, because it was dried before packing in vacuum bag)
@Exstaz3 жыл бұрын
@@MyTechFun i doubt it will affect the result much since it is tested over a period of time. It will absorb moisture and get soft. Directly after it was printed the piece that was printed with wet nylon would prolly lose.
@leeparsons703 жыл бұрын
Great test you done there. Very thorough . I thought why is ABS not there. Then later you said why. Well done. Did you think these results would have been any different?
@MyTechFun3 жыл бұрын
ABS is similar to ASA, but I am curious is there any difference between 4 most popular brands, that will be tested
@avejst3 жыл бұрын
Great test, interesting results I love your screew test, very visualy apealing I think the Nylon (PA12?) gives a strange results, I dont belive it is only Nylon in that filament! I use mostly PETg in my prints At work it is PETg and some ASA (For outdoor use) Thanks for sharing your expirences with all of us :-)
@MyTechFun3 жыл бұрын
There will be more testings in this topics. Few SLA comming soon, then eSun PC, PA, ABS+ then 4 ABS brands etc..
@adamrak7560 Жыл бұрын
At room temperature, I have experienced significant creep with PLA during a year. It permanently deformed until it broke, well under its tensile strength.
@WafflerSupreme3 жыл бұрын
Thanks for conducting the tests. I have a question regarding the torque test. Your data shows that ASA on day 2 achieve an a average angle of 66 and then on day 4 it’s 30 degrees and when heated it’s back up to 65. Actually it looks like your day 4 averages for all materials appears to be better. Any ideas on what the cause might be?
@MyTechFun3 жыл бұрын
I think that's normal. If there wouldn't be heating, that rotation angle would be smaller and smaller after every test, since the material is more compressed (this was printed with infill, as I mentioned). With heating, this angle jumps, but then it would be again smaller and smaller after every tightening.
@kilosera3 жыл бұрын
I modded my ender 3 to dual belted Z. Bottom belt holders were first from ASA and cracked a bit due to weak design (except the crack they were working fine). I reprinted buffied ones with PETG as I ran out of the ASA. I noticed that initially I had to spend more time leveling the bed than with ASA ones. Also now after few months I had to re-level the bed a bit. So at the next printer service I will replace the buffied PETG parts with buffied ABS ones.
@MyTechFun3 жыл бұрын
Thanks for sharing your experience, very useful info.
@robertbedsole86822 жыл бұрын
Great work & valuable results! Thank you! For C-ring test, maybe you could modify sample and/or fixture so top ear mounts to fixed bar. Then measure lower ear to bar (similar to cantilever flex test between sample & fixed table) Cheers!
@rico36962 жыл бұрын
Super video! Small improvement: when testing the retightening. Don't clamp both nuts at once. I think since this does not only lock the nut from rotating but also in vertical direction against the other nut.
@MyTechFun2 жыл бұрын
It is important to lock only nuts, to prevent them from rotating. So all rotation is made is visible (and measurable) from the other side. If I would hold only one nut, 3d printed object may rotate too during testing.
@rico36962 жыл бұрын
@@MyTechFun yes true! But I mean only one nut? Unsure
@rico36962 жыл бұрын
@@MyTechFun nevermind, with only one nut clamped, you could not messure the rotation since the part itself maybe turns as well
@Adam-ee9lm2 жыл бұрын
MyTechFun: did you post the follow-up video about different ABS's you're going to use for your voron ? i'm very interested in what you chose and tested there !
@MyTechFun2 жыл бұрын
Not in one video, but I tested eSun ABS+, ASA, Polymaker in separate videos, but results are comparable with each other. www.mytechfun.com/videos/3dprint
@zdenekvalek15383 жыл бұрын
Very interesting. Maybe test ASA with 3 ABS materials to have comparison. I am looking forward for ABS as it is the only material I print.
@Dramaican883 жыл бұрын
Great video and glad to know you are building a Voron. I am building myself a 2.4 300mm spec also. For the 4th ABS in your tests I can highly recommend "3DJake niceABS" or "Formfutura TitanX". I have been using 3DJake niceABS for my Voron parts, it is really good! There is also the option for "Amazon Basics ABS" which is cheap and I think more difficult to print, as it is not modified (no ABS+, ABS plus, ABS Pro, ABS no warp etc) it is just regular ABS, but it might be surprisingly good in properties because it is not modified. Finally, I would be interested to see NonOilen compared to PLA, especially because of the results in this video for PLA after heating and your previous video where you boiled NonOilen. I bought NonOilen from 3DJake because of your video by the way.
@MyTechFun3 жыл бұрын
Hm, that would be useful info, yes nonoilen resists high temperatures. So far, i was only thinking about nonoilen for food safe applications on my workplace (food engineering department). But from the other side, it is very expensive material, so I would prefer ASA instead (if no need for food safety). Oh, so many tests to do...waiting in a row.. pity that creep test is so slow process :-)
@plastikbeau36953 жыл бұрын
Thank you sir, very informative video. I believe all the impact tests in the world are kinda useless compared to this because most functional printed parts are just holding something, silently deforming over time. For even more comprehensive creep test I would like to see how part thickness influences creep for a given material. (So, for example, maybe PETG creeps more than ASA in a 2mm thick part, but less in a 6mm part) Another test would be to measure twisting creep.
@MyTechFun3 жыл бұрын
Twisting creep - great idea, thank you for the tip. Thickness effect to creep.. not sure if I will test that, more likely I will test is the correlation between thicknes and stress linear as with metals.
@koenvanduffel20843 жыл бұрын
Great test! All 3 the methods show similar results (though not always the same magnitude but that is to be expected). What isn't recorded in the state after taking the stress away. At the end of the video it is clearly visible how much elasticity is lost by PLA after just a short heat cycle. But I am surprised that Nylon is so poor and doesn't return to its original state. Polycarbonate is known to be very creep resistant but is brittle and sensitive to oils so would be a poor choice for your Voron build. PC-ABS might be the ideal material upping some properties of ABS (ASA) but not being so brittle as PC itself. That obviously leaves CF-PETG and CF-ABS or CF-ASA as options. The surely are stiffer and very creep resistant . Whether they don't become too brittle is a question.
@MyTechFun3 жыл бұрын
I just got from esun ePA, ePC and ABS+ so this will be one of my next testings. Carbon fiber...yes but a little bit later..
@martvansteenbergen8955 Жыл бұрын
I appreciate this test a lot as creep is an oft overlooked issue when designing plastic parts. However, and feel free to discuss, I have the impression this test is incorrectly setup because it does not account for the amount of stress relative to the yield stress of the material that the samples experience. For instance PLA is really known to creep a lot but because it is also strong and stiff, it does not deform greatly in these tests, since you are loading it with a different percentage of its maximum allowable stress than the other materials, which could be loaded closer to their yield points leading to increases in creep rate. The total amount of creep deformation at a fixed percentage of the material yield point would be more indicative, as well as the total deformation after creep recovery.
@SeanTaffert3 жыл бұрын
Great video. What about CF filled materials, especially PETG+CF, Nylon+CF or Glass Filled ASA?
@MyTechFun3 жыл бұрын
CF will be tested too
@StanEby13 жыл бұрын
Would like to see each sample bent the same distance of deformation for a week, then see which one returns more closely to it's original shape. Repeat it with heat.
@MyTechFun3 жыл бұрын
Something similar you can see in this video too, just before results summary.
@Sasha3153 жыл бұрын
Try to anneal PLA - grind table salt in coffee grinder, pack it around the PLA part. Put in oven at around 100 Celsius for 20 minutes. I tried it and PLA parts do become much stronger, though I didn't measure exactly by how much.
@MyTechFun3 жыл бұрын
I'll try annealed PLA too (comparison with regular PLA and Nonoilen filament). But not sure if I will anneal it in salt, I know it will deform but I will see the dimensions.. still new to annealing..
@Sasha3153 жыл бұрын
@@MyTechFun In my experience part doesn't change dimensions if packed in fine ground salt. You don't need to remelt the plastic, 100 degrees Celsius (212 F) is enough.
@santiagoblandon30223 жыл бұрын
Really useful information! Was the Nylon annealed? I've always wondered how much of a difference in creep of annealed vs un-annealed PA would there be
@MyTechFun3 жыл бұрын
Usually PLA is annealed, never heard about nylon annealing. The problem I have with annealing, is that objects deform a lot, not good for mechanical parts
@santiagoblandon30223 жыл бұрын
Nylon is semicrystalline and changes properties so much when annealed that manufacturers often times publish both datasheets, un-annealed and annealed. The reiforced versions (glass filled, carbon filled) can be annealed even at Tc without suffering dimensional inestability. For the unfilled versions, because the HDT is so high compared to Tg, the deformation annealing at Tg or a little bit above Tg is not too noticeable
@santiagoblandon30223 жыл бұрын
Oh.. and when annealing at Tc, the time period is much shorter. You can place a natural color sample of the same polymer with a similar wall thickness next to the part you're annealing and see when the indicator sample gets opaque, that let's you know the if crystallinity has increased. You can get different degrees of crystallinity, but I haven't tested that too much.. just got to see different levels of opaqueness and subjectively percieved different properties, but yeah.. I can't assert anything in that regard
@joshsekel3 жыл бұрын
For the compression test, maybe the results would be more useable if aggregate result was calculated? That would show how much in total the bolts had to be tightened.
@MyTechFun3 жыл бұрын
Yes, I agree, I noticed that later, now they are different type from first two. But, at least, excel table is downloadable, so it can be done by user too (*I will add this graph to downloadable excel)
@quelixfenzer51082 жыл бұрын
Thanks for the helpful information. I wonder how PLA would perform after heattreating. It probably wouldn´t spike that bad from heating but i wonder if the general creepresistance would go up or down
@Hyratel7 ай бұрын
screw clamping test shows the progressive creep, and how *at room temp* all samples had a high initial creep that then slowed down, but none were able to retain a clamping tension over time
@ztynzo3 жыл бұрын
In my V0, chamber temps are around 60C, I'd recommend setting that as an temp goal for testing, and I'd test over a 24hr period, as 2hrs at 45C doesn't compare with most of my prints. Good methodology though!
@dangerous83333 жыл бұрын
He's explained that 45°c is plenty to print ASA in an enclosure. So that's his goal. Sounds like you have a different setup. Maybe you should do the test yourself. Edit: Consider also if you have fume extraction your chamber temps aren't going to stay at 60c unless you have a heating element.
@LightSpeedIII3 жыл бұрын
I think for the screw test, the better visualization would be to show the running total angle, so day 1: 30°, day 2: you get another 50°, so plot 80° and so on
@MyTechFun3 жыл бұрын
That was my first plan, but pointers are too big, they will hit the other bolt. But I need two screws to lock the position of the nut on the other side. I can redesign the graph, so it will show summary result. I'll upload this graph to my website, link in description.
@LightSpeedIII3 жыл бұрын
@@MyTechFun ah, I think you can just add it on the graph, you don't have to do it with the pointers
@MyTechFun3 жыл бұрын
@@LightSpeedIII added, new excel table uploaded
@sandy.sasmita3 жыл бұрын
Can you make a video about 3d printed hose fittings / tap fittings like double nipple or connector, and compare how strong the material againts water pressure. PLA, PETG, ASA, Nylon etc. 100% infill or 100% perimeter. Thank you.
@MyTechFun3 жыл бұрын
I already printed some fittings for my fathers pesticide sprayer (1 bar) from PETG and it works now more than 2 years. But yes, this would be very interesting test.. great idea, thx.
@difflocktwo3 жыл бұрын
How much can we avoid creep by designing to lower stress? Maybe using more of a cheaper material is equal to less of a more expensive material.
@MyTechFun3 жыл бұрын
I don't know yet, this is my first creep test. But a good subject for future testing.
@difflocktwo3 жыл бұрын
@@MyTechFun Yeah, material is one thing and geometry another.
@logicalfundy Жыл бұрын
Printed a filament guide in PLA+, but it warped to the point where it wasn't really doing its job - probably because I print in an enclosure with elevated temperatures. So I've reprinted it in PETG, hope that lasts a bit longer. If not, I might have to add a rib to the design to stiffen it. I don't really have the capability to print some of the other materials at the moment, mostly need to figure out ventilation.
@testboga5991 Жыл бұрын
Could you do the same for a wide range of resins? It seems to be that all tough resins in the market creep like crazy
@MyTechFun Жыл бұрын
Hm. Good idea. I am curious now
@marcus3d3 жыл бұрын
It would be nice to see results of PP, too
@runklestiltskin_24073 жыл бұрын
Awesome, thank you so much.
@originalradman94913 жыл бұрын
Thanks!
@MyTechFun3 жыл бұрын
Thank you! I am glad, you find this video useful!
@dinosoarskill173 жыл бұрын
Have you considered carbon parts or glass infused filaments?
@MyTechFun3 жыл бұрын
Yes, sure, step-by-step. Carbon fiber filaments will be tested too.
@shvirik3 жыл бұрын
Great job! Please, check for the next test a 870 PLA filament.
@MyTechFun3 жыл бұрын
Hm, not the first comment who also suggested this. What is so special about this PLA?
@shvirik3 жыл бұрын
@My Tech Fun There are some youtube videos with 870 pla test,... it's look like "better" than abs, and obviously is easier to print. So, if we have a durable material and not hard to print, the non profesional printers (as me) have a good material to avoid the problems with other filaments. Děkuji :)
@MyTechFun3 жыл бұрын
@@shvirik Thx. Sounds like the Nonoilen, which I already tested (only not the strength, but the temperature, it can be even boiled or heat up to 110°C)
@shvirik3 жыл бұрын
@My Tech Fun Yeah ... it looks similar, but I won't use the water to make a tea :) The 870 also performs better with the heat: kzbin.info/www/bejne/q36sl4hqpMeZpZo (an example) Taking into mind that an 870 PLA could be bought for around € 22 / kg ... I think it is reasonable to use it for parts that should be durable without making your life difficult. (for printers noob as me).
@Kekht3 жыл бұрын
Cool video. But please do not hurry with Voron, wait for Vostok, or at least look at RatRig V-Core 3 :)
@MyTechFun3 жыл бұрын
I couldn't find any information about Vostok. Another Russian development, like Voron? (means East) *update, I found it, it will be Idex printer, but far for finished product v0.4
@DanCycles5 ай бұрын
Did you test this with Nylon 6 CF and Nylon 12 CF? I would love that test
What about polycarbonate? PC in my experience is very elastic, but also rigid.
@MyTechFun2 жыл бұрын
PC is tested in this video: kzbin.info/www/bejne/mZKzdqOVaNp7pac
@gitss73673 жыл бұрын
great information thank you
@Krealityfabrication3 жыл бұрын
Good learning, Thanks
@joshua432143 жыл бұрын
The screw test is extremely valuable, but there are 2 major issues with you current set up. First, the torque is way to high. This is the sort of torque you would apply to something like metal, not plastic. Second, the second torque is clearly being affected by the first. The screw holes need to have a division between them to absorb deformation - like the grooves put in concrete sidewalks. There are very good affordable dial indicators out there. In the US, Shars carries really nice ones that take a fair bit of abuse, and are accurate and repeatable. There should be an outfit that sells quality Chinesium stuff somewhere in your buying zone. Look for the places that hobby machinists get tools, not the places that Makers do (they are clueless about this sort of stuff). I would not buy digital unless you had some really compelling reason.
@MyTechFun3 жыл бұрын
You are right about screw test, I'll insert a groove between. What should be the torque for M5 in plastic? I'll buy dial indicators and rebuild the test setup a little bit
@BeefIngot3 жыл бұрын
Wish some carbon fibre petg was in this, though I imagine petg will say something about this Also Polycarbonate as an alternative to ABS, due to the no fume printing.
@MyTechFun3 жыл бұрын
There will be PC, PA, Carbon fibre etc materials. As I mentioned, this is just my first test to see the Creep specification for these basic materials. And also I am still searching for optimal creep test method..
@joshsekel3 жыл бұрын
Happy to hear there will be PC+ in future tests. I find it to be a very nice material to print and the temp resistance and strength is very good, but not sure about creep (until you inform us that is 👍).
@Deneteus3 жыл бұрын
Excellent!
@guate62 жыл бұрын
Appears ASA and PETG fared the best.
@Sportdue55 Жыл бұрын
Incredible!
@Javii966 ай бұрын
I thought your aluminum clamp to capture the dimension was a great idea
@alexvmw Жыл бұрын
greate work! thanks!
@Peter_Schluss-Mit-Lustig3 жыл бұрын
It seems your Nylon was quite Wet in these tests, at least it appeared quite fuzzy to me
@MyTechFun3 жыл бұрын
Yes, it was dried before placing in vacuum bag, so I dried it only few hrs before print, but looks like, was not enough
@Peter_Schluss-Mit-Lustig3 жыл бұрын
@@MyTechFun it probably would have been enough but nylon will "expire" in just a few hours in open air. somtimes even in the middle of a print
@OldCurmudgeon3DP3 жыл бұрын
At half way through, I might see one issue. I don't know the climate there, but I noticed the test pieces were sitting on the table in direct sunlight.
@MyTechFun3 жыл бұрын
Climate: inside 22-24°C. out approx 15-20°C day temperature. Effect of the sunlight is not too strong any more.
@JohnVanderbeck29 күн бұрын
So wait, everyone keeps telling me how bad PLA is at creep yet from skimming this video it seems better at creep than PETG which is what people keep telling me to switch to. Am I misunderstanding the results?
@CapuletPoeChannel3 жыл бұрын
28:05 yellow =PLA orange = PETG blue = nylon white = ASA green = ???
@MyTechFun3 жыл бұрын
Green is PLA but not creep tested. I was experimenting with dimensions on this filament as explained earlier.
3 жыл бұрын
in my opinion, there is no point in doing such long tests, test more: ABS vs ABS + vs ASA different PLA company from PLA + / HT-PLA ... and take the average for a given type of filament because there will definitely be differences and resins of various companies, ordinary vs transparent vs ABS-Like vs PLA (average) nice measurement after raising the temperature = ideal for use in, for example, a car
@adamrak7560 Жыл бұрын
Nylon absorbs a lot of water from the air and becomes _lot_ more flexible. So basically your test with the Nylon was invalid, because you were measuring the change in elasticity and not creep.
@solventtrapdotcom66763 жыл бұрын
That wasn't creepy at all...
@thelightspeed3d7123 жыл бұрын
Igor, Prusament Carbon Fiber PC! That’s what I want to know!
@thelightspeed3d7123 жыл бұрын
CFPC from Prusament is easy to print and is really strong.
@giovannidesimmeo52763 жыл бұрын
Why Nylon for these tests... Nylon is almost a semiflex material... 🤦
@MyTechFun3 жыл бұрын
I included it as one of 4 basic 3D printing materials, for this first creep test.
@thai95032 жыл бұрын
Hello Igor
@TommiHonkonen3 жыл бұрын
oooof voron. I bought ratrig.
@MyTechFun3 жыл бұрын
What's the problem with ratrig? That's good printer too
@TommiHonkonen3 жыл бұрын
@@MyTechFun No problem. In fact I see benefits for ratrig that's why I got it.
@christopheryeung11 ай бұрын
Can someone tldr the results to me
@brisance3 жыл бұрын
Anneal the different materials and redo the tests.
@MyTechFun3 жыл бұрын
I will, but I don't like annealing, because the object deforms a lot during this process. Not good for mechanical parts.