at work theyre having me sand with 180 then orange trizact pad and then white trizact pad to achieve high gloss. I saw them do it and am unable to produce the same finish. I was told the 180 was most important, done it thoroughly and was wondering if you haveany techniques for the trizact pads or have any idea why I'm unable to achieve the same high gloss? thanks!
@deepeshbhardwaj15 жыл бұрын
Dear can you told how we remove sander swirl mark with shinning papers.
@zackbrumis78314 жыл бұрын
Pretty sure orange trizact is finer than blue.
@fnk1017 жыл бұрын
Hi, Is earthstone worktops solid surface & would i do this on them to make earthstone high gloss finish