Hi there. In our lab we tried ditching covering our teeth in putty in favour of using just using stone. The finished product was great except we had a problems with stone sticking to the margins. Have you ever experienced this? Any suggestions for how to prevent it? Is your stone topping 100% stone or is it a stone and plaster blend? Thanks!
@WAXBAE5 жыл бұрын
Mix half stone half plaster. Sticking may occur if the separation wasn’t done correctly. If sticking should happen try to put the dentures in ultrasonic bath
@luna7402 ай бұрын
2:30, I am confused as to what this step is?
@WAXBAE2 ай бұрын
Pressing the flask?
@chanyuxin331111 ай бұрын
Can i open the flask if i forgot to put separator as in 0:53 ?
@WAXBAE11 ай бұрын
You could after boil out but the problem is if you inject and forgot the separator as the acrylic will be stuck on the stone
@chanyuxin331111 ай бұрын
@@WAXBAE Meaning at the dewaxing stage before injecting the acrylic, even I forgot to use separator, I'm still able to separate the flasks right? Just that it's a bit harder?
@chanyuxin331111 ай бұрын
@@WAXBAE Meaning in my case where the acrylic is not yet applied and it's still in dewaxing stage, I still can separate the flask right even the separator is not applied? So sorry to ask but I'm too worried..
@professordiogodias5 жыл бұрын
olá, qual nome desse equipamento que esquenta agua?
@kirkland8002 жыл бұрын
What is the brand/type of boil out tank you have there?
@WAXBAE2 жыл бұрын
Labormat
@achrafelkassih29303 жыл бұрын
what is the temperature of water for cooking the acrylic....thank you
@WAXBAE3 жыл бұрын
Always 100c
@AnilVerma-dy6jr3 жыл бұрын
Of course this is a modern techniques but in my opinion conventional technique result are same
@WAXBAE3 жыл бұрын
Now this is not considered modern anymore, digital is