Super Alloy 1 contains cadmium. An antique pot metal table leg that's been broken in half is repaired with a propane torch and multi-metal solder Super Alloy 1.
Mike explains how to build up the heavy piece of pot metal, to join the broken pieces at 20,000 psi. He then turns the part over and repairs the other side using Super Alloy 1 and Heat Freeze Heat Paste (formerly Cool Blue)
Pot metal and zinc diecast have almost a lead weight to them. If the part is light in weight to the mass of material it is most likely cast aluminum. Super Alloy 1 does not work on cast aluminum.
Heat Freeze eliminates re-melting of the original solder and also acts as a jig to hold the part in place while making the repair.
Always clean your pot metal and zinc diecast just prior to soldering the part. These metals oxidize quickly. The old saying is, don't clean it the night before, clean it right before you solder. Heavier sections like this part needed more preheating than most parts. Always heat the area adjacent to the section to be repaired. This will help the solder flow out flatter and will stay warm longer.
The Super Alloy 1 melts at a low temperature to prevent your pot metal from being ruined when soldering. Follow the tips and techniques in our videos and you should never approach the melting temperature of the parent metals.
Clean the flux residue off the rod before returning it to the PVC tube.
#HeatFreeze #JigPaste #RepairPotMetalParts #RebuildPotMetal
Please read all instructions prior to use at: www.muggyweld....
www.muggyweld....
For more videos and information, or to order, visit www.muggyweld.... or www.muggyweld....
_________________
Please visit www.aws.org/tec... prior to using Muggy Weld products, and adhere to all AWS welding safety guidelines. Further product safety information is available at muggyweld.com/s....
Muggy Weld LLC shall not be liable for any loss, injury, claim, liability, or damage of any kind resulting in any way from (a) your use of this Site, (b) any services or products obtained from this Site, (c) any errors in or omissions from this Site, (d) the unavailability or interruption of this Site or any features thereof, (e) any content contained on this Site.
MSDS sheets available with purchase from MuggyWeld.com, upon request.

Пікірлер
Inside Out 2: ENVY & DISGUST STOLE JOY's DRINKS!!
00:32
AnythingAlexia
Рет қаралды 18 МЛН
إخفاء الطعام سرًا تحت الطاولة للتناول لاحقًا 😏🍽️
00:28
حرف إبداعية للمنزل في 5 دقائق
Рет қаралды 76 МЛН
Когда отец одевает ребёнка @JaySharon
00:16
История одного вокалиста
Рет қаралды 13 МЛН
РОДИТЕЛИ НА ШКОЛЬНОМ ПРАЗДНИКЕ
01:00
SIDELNIKOVVV
Рет қаралды 3,8 МЛН
Aluminum Welding Rods: What You NEED to Know
4:31
Mr Fred’s DIY Garage School
Рет қаралды 283 М.
How to ID pot metal , white metal , cast zinc , monkey metal
11:21
HappyScrapper
Рет қаралды 13 М.
Repairing Pot Metal & White Metal using HTS-735-11
11:27
Aluminum-weld.com
Рет қаралды 13 М.
How to solder
7:23
House of Hacks
Рет қаралды 45 М.
The Secret to Soldering Brass
7:38
Diamond Mounter
Рет қаралды 41 М.
The BEST Metal Casting Alloy That Everyone Ignores
9:24
Paul's Garage (Paul's Garage)
Рет қаралды 360 М.
Inside Out 2: ENVY & DISGUST STOLE JOY's DRINKS!!
00:32
AnythingAlexia
Рет қаралды 18 МЛН