DO NOT OPEN THE BATTERIES THEY ARE HIGHLY EXPLOSIVE! PLEASE PUT A WARNING!
@RohitAllExperiment
@RohitAllExperiment 10 ай бұрын
What you are saying is true but there is not much umpire left in this battery, because of this there is no danger to us even if we pay attention to safety.🙂
@OrangeOrangutanSir
@OrangeOrangutanSir 10 ай бұрын
This is very dangerous since you are opening a battery.
@GadgetsHole777
@GadgetsHole777 11 ай бұрын
Can we used bleach please reply ❤❤
@adityasingh9126
@adityasingh9126 Жыл бұрын
Flux name
@joshielectronicsoundsarwar3084
@joshielectronicsoundsarwar3084 Жыл бұрын
भाई पेस्ट बना रहा है मुंह से तो सही बोल तोतला क्यों बोल रहा है
@SONUAGGARWAL
@SONUAGGARWAL Жыл бұрын
Wo muh me thora flux chla gya tha
@rahulbhaskar4179
@rahulbhaskar4179 Жыл бұрын
Good only for beginners....
@GangaRam-h5i
@GangaRam-h5i Жыл бұрын
Bad teach. Bad teacher
@kalidashsikder
@kalidashsikder Жыл бұрын
Acid ka nam kiya hay????
@xbillygangx
@xbillygangx Жыл бұрын
Hydrochloric Acid نمک کا تیزاب
@Sanju220-t2k
@Sanju220-t2k Жыл бұрын
Subscribed 💝😍
@Sanju220-t2k
@Sanju220-t2k Жыл бұрын
Rohit ji aram Malta safty first . Bhut mast Apne to hath hi krab kar liya mre bacpan ki jese hum bhi cell ko tod ker dek deki karte thy. Ye light ata kese h😍
@opposites-369
@opposites-369 Жыл бұрын
This hindi way, always thought you with danger method
@caribbeanguytrinbago9662
@caribbeanguytrinbago9662 Жыл бұрын
what was in the cup ?????????????
@RohitAllExperiment
@RohitAllExperiment Жыл бұрын
Meera banaya wa shouldering flux
@dilipmarathe3439
@dilipmarathe3439 Жыл бұрын
I tried ad per this vedio but not good quality flux. For you have to use sulfuric acid. Uhave to tske care while making flux. This acide is very hazardus. Make this in open space where high air flow. It gives high smoke so keep away from you till lid material gets fully melted. Always wear had glows while working. Then you get good result.
@debkumar9955
@debkumar9955 Жыл бұрын
Thanks
@amorsoloarts
@amorsoloarts Жыл бұрын
What chemical did you used?
@RohitAllExperiment
@RohitAllExperiment Жыл бұрын
Sarah Cleaner Acid.
@MukeshKumar-hp6rb
@MukeshKumar-hp6rb Жыл бұрын
Kya bataya he
@manishytgaming4908
@manishytgaming4908 Жыл бұрын
Nice video
@debkumar9955
@debkumar9955 Жыл бұрын
@Startradelink-p1g
@Startradelink-p1g Жыл бұрын
H2so4 1250 gravity + NaCl,Namak, me 24hrs gholne se Banta hai.
@debasishdas777
@debasishdas777 Жыл бұрын
😮👌...
@himkargupta4348
@himkargupta4348 Жыл бұрын
अरे भाई अगर छुपाना चाहता है फिर बनाई काहे को वीडियो
@RohitAllExperiment
@RohitAllExperiment Жыл бұрын
अरे भाई मैंने इसमें सब कुछ बताया है
@RohitAllExperiment
@RohitAllExperiment Жыл бұрын
Shera Cleaner
Жыл бұрын
What type of acid did you use to melt the metal of the battery? Thank you
@thomastrzepacz9614
@thomastrzepacz9614 Жыл бұрын
sulfuric acid is used, looks like he used drain cleaner with sulfuric acid. lead batteries contain this mixed with water.