1. 0:00 Intro
2. 0:19 Pinholes on ceramic surface ater firing
3. 1:28 Temperatures & improper drying process of the application
4. 4:02 Excessive amount of organic material (inside the inks)
5. 5:50 Chemical incompatibility between engobe and grit (or glaze)
6. 7:11 The firing cycle: an untouchable variable
7. 8:40 Conclusion
After the ceramic body forming stages and the following digital printing steps, the ceramic production process involves a final application of grits or glazes, sometimes in significant amounts. Failure to apply the correct process parameters can sometimes lead to issues in this application, which can compromise the ceramic surface in a number of different ways, from both an aesthetic and technical perspective.
See more: www.zschimmer-schwarz-ceramco...