well that sucks... this sounds simliar to 80s 90s clearcoat delaminaition where factory paint jobs were being mixed incorrectly or not waiting long enough for the base coat to degas before applying clearcoat... hope when you do it again it works as it should since it's their fault for giving you the wrong tech sheet are they giving you a break on the paint they absolutley should take the blame and help out.
@MetalMania3DTV-TAS-AUS3 ай бұрын
Totally agree with you there 💯 percent 😊
@ramblers693 ай бұрын
You're going to need a bigger purple pond 😂
@woodysmodels87383 ай бұрын
That for sure lol.
@garyparker29693 ай бұрын
I'd Take HOC To Court For Miss information, 2 paint jobs, Labor For 2 paint jobs and Mental Anguish + Whatever You Can Think of 🤬🤬‼️ Have a Blessed " Memorial " Wknd Buddy 🙏🤗 Gary.
@woodysmodels87383 ай бұрын
Thanks Gary but it wasn't HOK fault it was the paint salesman but I have spoken with them so see what happens