Does anyone know a good KZbin channel or a website for quick construction tips like this?
@gurwindersingh-ug5ty6 жыл бұрын
sir how many time tapping rod in slump cone
@civilengineeringconcepts88985 жыл бұрын
25 in 3 layers or 5 layers
@ablet854 жыл бұрын
But don't do it like they did. As you pour the concrete in you are supposed to rotate the scoop. With the 25 per layer it isn't supposed to go through that layer.
@tom195810002 жыл бұрын
25 times.
@maaroufchetitah3054 жыл бұрын
Good
@Timliu928 жыл бұрын
That is too much water for the slump. The mix proportion now needs to be adjusted to get a true slump that is desired for construction.
@هابعلي7 жыл бұрын
Bad concerteYou must reject this mixture 😁
@Ihsanmeerani7 жыл бұрын
How to know the ratio if we know kgs of proportions like 470 kg cement 707 kgs sand and 962 kgs aggregate
@tom195810002 жыл бұрын
Usually each concrete truck must comes with a ticket from the plant with the mix ratio for that exact truck mix!
@Kellyc428 жыл бұрын
that asshole driver fill that wheelbarrow completely full, i would have dumped it and gotten another sample
@chaudhry51307 жыл бұрын
It doesn't matter
@tom195810002 жыл бұрын
It's not up to the drivers to give what they want to the tester, It's up to the tester to ask for how much they need to test.
@AnuragSingh-kt3on7 жыл бұрын
To much water be filled in the concrete
@rupeshgavand44492 жыл бұрын
for More videos of Civil Engineering Testing Equipment please click here - kzbin.info/www/bejne/oYm1Xmpnbst_mdE
@rameshmali58544 жыл бұрын
Collapse Slump indicates water cement ratio is too high
@gkcool9347 жыл бұрын
that's totally filled ...
@zeeshanahmad-fb4zx7 жыл бұрын
Collapsed don't allow these type of concrete
@basha.eliyas41295 жыл бұрын
Zero slump
@claudreindl72756 жыл бұрын
Bad slump test shown with voids in concrete. Proper rodding eliminates voids and provides consistent tests. What you show is crap!
@lubradoon8 жыл бұрын
Too much water
@sgs33317 жыл бұрын
s
@abedserhan20547 жыл бұрын
Weak mixture
@shaikmasoodali95526 жыл бұрын
the testing lab didn't test it properly, he removed the cone abruptly.. i have read somewhere in american code if super plasticizer is used, the slump can b allowed upto 20cm for vertical members..
@himanshukhatwani55578 жыл бұрын
Failed
@divakarsr82995 жыл бұрын
bad concrete, method of testing is also not in proper way, waste video