Nice work, i have learnt a lot from your video. Thank you
@ImranShaikh-kl7mj4 жыл бұрын
Thanks for your video they are so informative and I learned allot from your videos
@edeminamessienobom63275 жыл бұрын
thanks so much for the lecture, i have learnt something
@besttoursenterprisess.a.52146 жыл бұрын
I had to stop the video part way through just to say thank you. This was a very informative video. I learn a lot from your videos. This one I must admit was exceptional! It was definitely worth watching again. "My wish list?" More videos on chillers.
@geerthenkwijnants8 жыл бұрын
No reference tubes, not any note's being made. Only single channel (differential) automatic registration. Normally an absolute channel is required for interpretation purposes of anomalies encountered. Having no note pages seems odd since normally you'll always encounter some particularities that need further investigation.
@IAMKUNLEOLUSESI Жыл бұрын
Do you have paid training Ken? How much does it take to perform an Eddy current testing on a 800 tons Chiller?
@KenTraining Жыл бұрын
Thank you for asking but I do not.
@bobd32464 жыл бұрын
Very well done video, easy to understand. I have 4 very similar looking York chillers that are 200 tons each. The condenser and evaporator supply and return lines are on the same side though. What size are the chillers in the video? I'm also assuming they are York, correct?
@mikeyangel10676 жыл бұрын
I’ve watched many of your videos and wanted to thank you so much for taking time to explain. My school did not address chillers or commercial hvac issues as much. Any books you recommend. Tnx
@บรรพตสอนดี4 жыл бұрын
Thank you
@antinmenus763 Жыл бұрын
If have any eddy current testing job vacancy
@maplic4 жыл бұрын
Quite low fill factor on that ET probe. Hopefully that's not underfinned and you guys aren't looking for small diameter defects!
@darshandipalidilipdudhane10774 жыл бұрын
Dear Sir, why we are set hole on 40 degree and 1volt for differential channel and why we are set absolute channel 0.1 volt at 40 degree for internal tube inspection by bobbin probe. Can you please explain it
@alexwhite20313 жыл бұрын
Ir depends on the code he's working to... he may have a more lenient code where only larger discontinues are rejectable.. at least I'm assuming that's why hes using a UniWest instrument opposed to something more advanced like a corestar.
@raymiles6913 жыл бұрын
This I guess is some of what my father meant in mentioning ED. (savvy😐 ?)
@s.umarfasith347410 ай бұрын
Any job vacancy available
@KenTraining10 ай бұрын
Not that I know of but Thanks.
@peteygr9 ай бұрын
nice video. Maybe mention the correct spelling of learned is not "learnt"
@chrislowe88317 жыл бұрын
is he even recording...i want to know the condition of every single to be on my trane..
@chrislowe88317 жыл бұрын
tube *
@justincarpenter63622 жыл бұрын
Prime example of how to not do eddy current, acquiring bad data, antique machine, pulling too fast for CuNi, bad tube designation...if any at all.... smh.
@russellbarnes77322 жыл бұрын
Justin, it looked like he was not going all the way down to the end of the barrel. Also Did not look like he was mapping the tubes so that he would know which tube needed to be replaced If you found a thin one