In this video, I have explained the acceptance or rejection criteria of welding defects in power piping as per ASME B31.1 code.
The weld defect acceptance/rejection criteria are given in Chapter VI (Inspection, Examination, and Testing) of the ASME B31.1 - 2022 code.
In chapter VI of ASME B31.1, the Qualification of NDE Personnel and the acceptance/rejection criteria for the weld defects by the following examination methods have been given;
1. Visual Examination (Para 136.4.2)
2. Magnetic Particle Examination (Para 136.4.3)
3. Liquid Penetrant Examination (Para 136.4.4)
4. Radiography Test (Para 136.4.5)
5. Ultrasonic Examination (Para 136.4.6)
6. In-Process Examination (Para 136.4.7)
Join this channel to get access to the perks:
/ @weldingandndt
*******************************
*******************************
Here is a list of the top 5 performing videos on my KZbin channel;
1. MIG Welding: • [Hindi/Urdu] MIG Weldi... (8,00,000+ Views)
2. Welding Positions: • welding positions 1G, ... (6,00,000+ Views)
3. Shielded Metal Arc Welding: • [Hindi] Shielded metal... (4,70,,000+ Views)
4. Types of Steel: • [Hindi] Types of Steel (3,70,000+ Views)
5. TIG Welding: • [Hindi] TIG Welding - ... (2,50,000+ Views)
*******************************
*******************************
Connect With Me;
Website: www.weldingandndt.com/
KZbin: / weldingandndt
LinkedIn: / sandeepanand27
Facebook: / weldingandndt
About me: www.weldingandndt.com/about-me/
Email ID: weldingandndt1(at)gmail.com
Please subscribe to my channel and share the links with your friends and colleagues on social media such as Facebook, WhatsApp, Telegram, and Twitter.