The first phase of gilding is applying the gesso. The video shows how to prepare the gesso and how to apply it on the frame.
Пікірлер: 27
@Bluebuthappy1827 жыл бұрын
I'm only the first lesson here but I'm thinking if i was a rabbit I'd be a little bit nervous. Excellent videos by the way.
@Davidhandles243 жыл бұрын
The surface that I am gilding is a smooth sealed surface not porous do I still need to gesso or can I just add the bole on top
@padgecrack40186 жыл бұрын
No, the first coat is called colleta . It's a layer of pure rabbit skin glue. And it's usually more than five coats of gesso!
@gildingstudio6 жыл бұрын
Indeed :) I go from 14-25 coats by hand.
@Davidhandles243 жыл бұрын
I purchased a premade gesso that contains rabbit skin blue and white team just don't know how much water to add to this what Do you think the ratio should be
@palanivel53332 жыл бұрын
Will you send me this gulu powder
@CoxJoxSox7 жыл бұрын
Wouldn't a paint work just as well today?
@gildingstudio6 жыл бұрын
No, it wouldn't. Gilder's Gesso, used for traditional water gilding, uses rabbit skin glue for it's strength and flexibility to move with the wood over time. The calcium carbonate works well as the filler allowing the gold to be later burnished. No gesso no burnish. Paint can be used, however, under oil gilding, a separate process for gilding.
@bobwilson59106 жыл бұрын
Rabbit collagen glue is very strong, but it has very poor flexibility in certain environments. Modern polymers are much more flexible and less likely to crack.
@gildingstudio6 жыл бұрын
Hi Bob, Modern polymers do offer benefits in areas of conservation, I agree. But rsg is used throughout the industry and its flexibility for use in gilding is one reason it's used. Stress crack mechanisms can indeed occur over time, mainly through fluctuation of humidity. Perhaps you're confusing the two methods of mordant/oil gilding with traditional water gilding. Kolner does offer an acrylic based system for water gilding but the traditional method has no comparison to any other method for gilding wood. Any paint medium under leaf would work underneath oil gilding which I also do but gessso with rsg, water, and calcium carbonate (or marble dust by some) is what's used for water gilding.
@padgecrack40186 жыл бұрын
There is a gold paint which can burnished.
@gildingstudio6 жыл бұрын
Depends on what you have in mind. As a decorative finish, traditional water gilding has no equal. There are simply things you can do with gold that is water gilded that cannot be achieved any other way with it's subtleties, warmth of tone and lack of oxidizing above 22k.
@padgecrack40186 жыл бұрын
It's not plaster. It's powdered whiting!
@hermanhermitz91016 жыл бұрын
Video is good but background music is completely unnecessary.
@moustaches17 жыл бұрын
Sorry not plaster it’s french chalk !
@gildingstudio6 жыл бұрын
Yes, a number of names we use but most common in the US is calcium carbonate of which there are numerous grades and particle sizes.