Amazing.... that drop of gold covered entire piece of that part.
@TrinityGoldRecovery Жыл бұрын
Indeed 😇
@reisonnuredini5495 Жыл бұрын
Great to you Trinity, nice job😊
@TrinityGoldRecovery Жыл бұрын
Thanks dear 😇🙏
@elektrotehnika8077 Жыл бұрын
Hello, can I dissolve legs from ic chips first and then incinerate them?
@chrisleigh6842 Жыл бұрын
hello, I want to create AR . I can only buy 25% HCL and 10% nitric acid or potassium nitrate.will this work? thankyou
@TrinityGoldRecovery Жыл бұрын
Yes, you can create a simplified version of aqua regia with 25% HCl and either 10% nitric acid or potassium nitrate. For nitric acid, mix in a ratio of about 1:2 (nitric acid : hydrochloric acid). If using potassium nitrate, dissolve it in water to create nitric acid. Exercise caution, use protective gear, and work in a well-ventilated area due to the corrosive nature of the mixture. Remember to prioritize safety!
@الخرباويخالد11 ай бұрын
مبدع دائمن اخي ❤
@oz-corner8281 Жыл бұрын
Great content and thanks for sharing! Looks like a good cost-effective alternative for lifting gold plating from RAM finger and other plated items. Can you speed up the reaction by heating? Cheers
@TrinityGoldRecovery Жыл бұрын
Heat can be applied experimentally.
@nevercertain Жыл бұрын
New Trinity video? Awesome
@TrinityGoldRecovery Жыл бұрын
Thanks dear 🙏😇
@OwlTech333 Жыл бұрын
Wow that’s must have been gold wrapped!
@TrinityGoldRecovery Жыл бұрын
Haha, if only! Maybe I should start a side business in gold wrapping too. Thanks for commenting on my channel, dear dude. Appreciate your honorable presence! 😇❤️