Thank you for your video. Regarding 0:40, the chemical formula for Potassium Cyanide is KCN. Caution must be used whenever handling cyanide, because cyanide could be fatally poisonous if it is ingested, inhaled or absorbed through bare skin. Regarding 2:25, combining 1 part nitric acid + 3 parts hydrochloric acid produces nitrohydrochloric acid, which is also known as Aqua Regia. Regarding 7:43 gold electroplating solution, if pure gold is used on the anode instead of stainless steel, then the gold electroplating solution will last much longer. This is because the gold cations in the electroplating solution will not become depleted since they will be replenished from the gold anode.
@expgame712 жыл бұрын
Is potassium cyanide mandatory for the proper functioning of the plating? Is it possible to replace it with another chemical element that is easier to find?
@jadenephrite2 жыл бұрын
@@expgame71 Thank your question. Gold electroplating can indeed be performed without the use of cyanide. Alternatives to the use of potassium cyanide is to use either sodium gold sulfite or to use potassium gold sulfite.
@expgame712 жыл бұрын
@@jadenephrite ok thank you for your reply. How to make sodium gold sulfite and potassium gold sulfite, is nitric acid needed?
@expgame712 жыл бұрын
@@jadenephrite yes but the problem with the solutions already made is that it is very expensive for very little gold, I would like to be able to make it myself
@aru_13962 жыл бұрын
What is the toxicity percentage of potassium cyanide used and what is the grade of KCN
@vishalsambrekar2 жыл бұрын
Thank you so much.i am goldsmith .i am watching everywhere,asking everyone bu they dont tell me how to make gold plating solution.your video is best instructor to me. thanks
@CrewDesigner-q7w24 күн бұрын
Sir have you applied this process
@nilshkmr24 күн бұрын
IF YOU DONT KNOW HOW TO MAKE GOLD SOLUTION THAT IS SUCH A BASIC KNOWLEDGE....THEN HOW CAN YOU CALLED YOURSELF A GOLDSMITH.. YOU MUST ME BLACKSMITH OR COBBLER INSTEAD
@vishwanathsah86573 жыл бұрын
No one explained like this well done bro
@vanjasemic81983 жыл бұрын
I cant believe!!!! Its wonderful!!! Congratulations
@AnifG3 жыл бұрын
Thank you so much 😊🙏
@PowerbyNFS3 ай бұрын
Hello sir , am very new in this business although I was checking out this video only & I found your video & knowledge , your idea made investment 90% less then what I actually thought❤
@marinnicolae42152 жыл бұрын
A nickel coating is required beforehand because the silver or copper atoms migrate to the outside and discolor the gold
@2ndPortal Жыл бұрын
Why, his attempt looked great. Are saying with time?
@travismiller5548 Жыл бұрын
Why nickel comes before chrome as well.
@lenny108 Жыл бұрын
Some say the best is to have chrome. On Amazon they sell gold electrolyte that is supposedly abrasion resistant. How is this achieved? Abrasion-resistant gold plating?
@RahulPatel-kk1ci Жыл бұрын
nickel or chrome coating is good but not good for the skin so avoid to do
@newmonengineering Жыл бұрын
@RahulPatel-kk1ci if you don't use nickel, the silver will tarnish under it and slowly discolor the gold. Most gold plated things are a very thin coating of gold. You can however go thicker to say 2.5 microns and it's a much better protection but also significantly more costly to do. Often they will use rhodium as a base layer over silver if they don't use nickel
@dongbotang3 жыл бұрын
Great video! Many thanks from Australia.
@AnifG3 жыл бұрын
Thank you so much.. greetings 🇮🇩
@nilshkmr24 күн бұрын
THANKS..... I LIKE THE WAY YOU DESCRIBED EVERYTHING I
@HR_SAINI2 жыл бұрын
You are teaching a masterpiece💗💗
@alejandrogracia44483 жыл бұрын
This is priceless, thank you so much! 🙏
@AnifG3 жыл бұрын
Thank you so much sir😊🙏
@cabulingue3 жыл бұрын
Terima kasih banyak Pak Anif G, Saya doakan bapak selalu sehat, banyak rejeki n berumur panjang teruslah bikin konten yang bermafaat. pak cara buat yg rose gold itu pakai campuran CU tadi ya, salam
@AnifG3 жыл бұрын
Amin.. terimakasih banyak om..🙏..iya betul om untuk rosegold saya pakai Cuso4/terusi.. atau bisa juga pakai yang sudah menjadi larutan
@machruskenzo73462 жыл бұрын
Thanks you very much 👍,,, good luck bro 👍
@MrMo7emad3 жыл бұрын
İ don't know how to thank you İt's very useful video
@AnifG3 жыл бұрын
You're welcome, sir 😊🙏
@Gazanferylmaz3 жыл бұрын
Will, we encountered a problem such as gold sinking over time?
@sirbinyamin76363 жыл бұрын
Hello, Can you let us know where did you get all the chemicals you are using? because in my country I try over and over but it is simply impossible to find them or they want to sell them by huge quantity... thanks 😀
@avivhanale31743 жыл бұрын
Hello sir can you tell me how to make brighter for this solution
@phool2893 жыл бұрын
Very easy to understand thank you so much 💝
@MetalGearIV2 жыл бұрын
wow you are a gift for humankind
@karangandhi52163 жыл бұрын
Hello sir, Thank you for ur vedio If we dissolve 1 gm how much gms we can polish for 24k
@kmcsmachinerytools26523 жыл бұрын
5000 grm
@ramujaisawal48212 жыл бұрын
Best
@nacholoyola84472 ай бұрын
Muchas gracias por compatir su conocimiento con nosotros !!!!
@leleaquino13122 жыл бұрын
Thank you for your video. In Brazil I didn't find any video talking about the chemical part of gold solutions How many times can this solution be used? Can I use up to how many grams of jewels without losing the gold?
@fireworkstarter3 ай бұрын
it can be used untill there is no gold left in solution, it will probably slow down on lower concentrations. if you put in 1 gram of gold into your solution you will very likely get 0.99 grams back. how much you use per jewel depends on how strong the electricty is you use, the surface area and the time you plate it for.
@pbjsilverstudio48823 жыл бұрын
Saved this video!! Thanks!
@AnifG3 жыл бұрын
Yes ma'am.. thank you very much 😊🙏
@safirjhnam9296Күн бұрын
مرحبا هل يوجد البديل عن ساينيد البوتاسيوم ؟؟
@sofiahearts46253 жыл бұрын
Best video thanks..........👍
@AnifG3 жыл бұрын
Thank you so much 😊🙏
@detectormaniaindonesia81312 жыл бұрын
Any working PH for this plating? Thanks
@johnkaka1000 Жыл бұрын
Thank you so much. It’s a great help.
@dusanstanic14623 жыл бұрын
Can stainless steel be plated and what is the procedure (preparation etc)? And how durable is this plating? Thank you
@dusanstanic14623 жыл бұрын
Where is the best place to buy gold?
@sachinlohar11063 жыл бұрын
Sir isme kitna kam niklta hai
@mochamadvidal41862 жыл бұрын
Mantap boss. Kalau boleh tahu, tinggalnya dimana..?
@manishkumarpatidar70003 жыл бұрын
VERY USEFUL THANKS.A LOT.
@sirbinyamin76363 жыл бұрын
Hello, does anyone know where to buy those products? A internet site or any other place would be really helpful. Thank you very much
@Themaker-studio Жыл бұрын
I don't think potassium cyanide can be purchased on internet. It's a very dangerous substance.
@StrengthAndHonorKnowledge4Life Жыл бұрын
Lab alley
@nilupul843 жыл бұрын
Hi Dear, I try it gold plating is really good. but something wrong in my solution. some brown dust making on SS Anode. can you tell me. HCL,HNO3,KCN & Water quantity for 250mg 24k Gold . Thanks
@anushkaverma68353 жыл бұрын
Hello sir aap kis country se
@AnifG3 жыл бұрын
Indonesia sir
@armazrivera23023 жыл бұрын
Can it be applied on pieces of steel ???
@AnifG3 жыл бұрын
No, it can only be used for gold, silver and copper
@armazrivera23023 жыл бұрын
@@AnifG If I cover the steel with copper, will it work?
@franknieto27603 жыл бұрын
Potassium cyanide is very deadly. Where can you get it? Other than gloves and good ventilation, what precautions should one take?
@AnifG3 жыл бұрын
yes it is very poisonous, I think a lot of materials for the jewelry production process are toxic, the important thing is to always maintain work safety with the right procedures
@armazrivera23023 жыл бұрын
There is an internet page where you can find potassium cyanide
@GILBERTOMARTINEZSAUCEDO Жыл бұрын
Hi! my stainless steel plate started to corrode during the plating process, and contaminated the solution (green/orange) sediment do you know why this is ?
@joonaskekoni28677 ай бұрын
You should have used titanium(?)
@ishqesahil88643 жыл бұрын
Is it suitable for stainless steel?
@sirbinyamin76363 жыл бұрын
As much as I know it is not possible to plate Stainlees steel
@lagosjewelryschool2765 Жыл бұрын
@@sirbinyamin7636 you can actually but it has its plating solution composition is different
@mohideenanver37002 жыл бұрын
Thank you so much for sharing plating process
@jaspergold45893 жыл бұрын
Please can you use 18karat gold to make the gold plating solution?
@AnifG3 жыл бұрын
Thanks for watching... I can't seem to do it
@randimadanthanarayana38392 жыл бұрын
Thank u sir. Its really helpful for me. Sir, i did this same as your video. And i plated. Rings, pendents. after plating its really nice and success. But it is not possible for chains. Chains are got black and very ugly colour. Can plz advice me sir.
@mohamadisham36039 ай бұрын
How you settle your chain issue ?
@pratishshrestha96233 жыл бұрын
How long does it last??
@chrissmith841 Жыл бұрын
Does it work out much cheaper making it yourself than buying ready made? thank you
@solmaz.khorashadi Жыл бұрын
Thank you for your helpful video. I have a QUESTION, is it possible to make the rosegold solution into rosegold powder?
@rajasasitepu953111 ай бұрын
Bang Anif, sdh like n subscribe. Saya sdh tonton video part 1 dan 2 ini. Makasih. Tapi nanya ini, apakah semua obat/zat kimia itu bisa dibeli bebas di toko kimia? Itu aliran listrik saat ngerendam cincin, pake brp volt itu bang. Thanks.
@hermanrany33253 жыл бұрын
Assalamualaikum bang, mau nanya. Bagusan mana sepuh merah dulu atau sepuh putih perak dulu sebelum proses sepuh emas?🙏
@Ans_Pro3 ай бұрын
Bisa Buat Pen Plating Kah Mas?..
@SultanSalmanVlog3 жыл бұрын
Bang numpang nnya juga ni sama ahlinya.. Kalao untuk pemerah harus pakai potassium cyanide.. ?? Yang berapa persen bang..?? Makasi infonya..
@Mayarfactory2 ай бұрын
Permisi om mau tanya apakah bisa di aply ke titanium?
@Midou542 жыл бұрын
please, if we want the color of green gold and blue for example, what sulphate is needed to achieve it, and a thousand thanks for this important video, I await your answer
@wacdiamondofficial3 жыл бұрын
Pak hanif. Kalau mau ngelapis emas di cincin berbahan stainless, ga bisa langsung kaya di video ya? Apa ada tambahan campuran khusus?
@AnifG3 жыл бұрын
Kalo untuk stainless gak bisa bang..ini cuma bisa untuk melapisi tembaga, alpaka, perak sama emas
@billmusik9794 Жыл бұрын
Is that just plane potassuim?
@tonykarlsson8589 Жыл бұрын
Good job 😊
@قناةالالعابالممتعة-ح9ث2 жыл бұрын
Thank so mach for this interesting video but i am just wondering of using potassium or potassium cyanide
@InfinityJewellery062 жыл бұрын
Can 14k gold be played in this solution
@ccezar843 жыл бұрын
Hello Anif. How thick can you plate with this solution without getting dull? Can you achive 2 microns of bright gold plating? This solution plate on non-ferous only? How good is the adhesion?
@AnifG3 жыл бұрын
Thanks for watching, I don't understand the answer to your question, but as far as I am it is the cheapest way to get the gold solution, and I always use it
@isawalter34653 жыл бұрын
can you please explain that ? I just know this channel and never saw, he says something about dumbness beyond 2 microns ... sorry german but the guy is super experienced .. kzbin.infovideos
@isawalter34653 жыл бұрын
@@AnifG Hi dear Anif, amazing! I am following this channel. He recommends 3micron for average use up to way more depening on purpose. Is your solution limited regarding micron thickness? thank you! Are you on Facebook for PN? thank you! :-)
@padmanavajethy7213 жыл бұрын
Good work. How to harden 24 carat gold. Any other metal could be used?
@AnifG3 жыл бұрын
Thank you so much..😊🙏 For 24k gold solution it can be used to coat various jewelry made of gold, silver and copper
@padmanavajethy7213 жыл бұрын
@@AnifG I am a goldsmith . I need to add some hard alloy with gold so that the gold coating becomes hard and the jewellery colour will last longer. Could any hard metal could be added to the solution?
@AnifG3 жыл бұрын
For the addition of other metals besides gold, of course you can't sir, this method is only for 99% pure gold which is dissolved, the environment mixed with other metals such as alloys will certainly damage the solution, but if you want to make the coating more durable you can use a nickel solution whose video I will for coming 🙏
@nyomanngetis6329 Жыл бұрын
Maaf boss, untuk sepuh rose gold apakah bisa buat ketebalan tertentu?
@bling66462 жыл бұрын
Hey Anif, Thank you for this rare video. How can I make a 14 karat gold solution?
@joonaskekoni28677 ай бұрын
I would assume mixture of zink cloride snd copper suphate. I however fail so see why anyone wanted that.
@hobiaja76663 жыл бұрын
Ada yg jual air sepuhan jadi tinggal pake nggk mas yg kayak itu.....? Terimakasih
@AnifG3 жыл бұрын
Di toped ada bang
@sagaspace3 жыл бұрын
Can we do gold plating of iron. I want to try on magnets. Is it possible?
@meowme76442 жыл бұрын
What magnets are of iron? You don't mean these shiny Neodymium magnets? Do you mean ferrite magnets?
@sagaspace2 жыл бұрын
@@meowme7644 no weaker magnet like fridge magnet neodymium are v strong.
@travismiller554810 ай бұрын
The neodymium magnets are already nickel plated, you're good to go
@ArshadAli-ny3dr3 жыл бұрын
Which metal is the ring you used? And can I do this color on aluminum
@AnifG3 жыл бұрын
It's silver...you can't use this solution for alumunium
@gonzalovaldez82043 жыл бұрын
Hello, it is an interesting process, when you brown a ring, the liquid that remains is discarded no longer works, how resistant is the gold, how do I make it last longer, I have seen you do other processes of black. as it does. can you teach me. saludos desde Colombia
@akhmadfazar70042 жыл бұрын
Kalo buat 100 potong emas brp takaran emas untuk di larutkan?dan talaran hno3 sama hcl nya jadi brp gan?🙏
@muchniksolo49802 жыл бұрын
@@akhmadfazar7004 biasanya dijitung dr berat mas yg akan di plaiting,aku sendiri jg buat dgn cara itu utk bahan emas 0,25grm dpt menghasilkan kurang lebih 1kg,semoga membantu🙏
@alexsinlae58763 жыл бұрын
Untuk gold colornya gmn ?? Makasih
@AnifG3 жыл бұрын
Untuk pewarna emas bisa pakai auruna bang.. tapi gak usah dicampur potas..cukup larutan emasnya aja..
@randyreyes8689 Жыл бұрын
Thank you for your video, thank you very much
@armazrivera23023 жыл бұрын
Hello Angie, how much water do you need? 0.5 grams or 1 gram
@AnifG3 жыл бұрын
For 1 grams of gold you need about 6 ml of HCL and 2 ml of HNO3
@armazrivera23023 жыл бұрын
@@AnifG thanks how many grams of cyanide potassium do I need and how many milliters of water to dissolve it I am about to do it I got 0.5 gram 24k gold
@flight36243 жыл бұрын
How to maintian the bath for large scale production of rose gold
@AnifG3 жыл бұрын
It is only suitable for small scale, for large scale production I have never tried🙏
@faisalishfaq58773 жыл бұрын
@@AnifG contect naber
@ishqesahil88643 жыл бұрын
Anif I want to gold plate surgical instruments. Can you please tell me what proportions of ingredients are used in yellow gold plating and what is the lifetime of this plating?
@jacquesomersavard72572 жыл бұрын
is it possible to make this whit stain glass copper frame or lead frame
@anandpanchal63903 жыл бұрын
Thanks for share your precious experience How much ml Hno3 and Hcl for 2 gram gold
@AnifG3 жыл бұрын
for 2 grams of gold, you need about 10 ml of HCL and 3 ml of HNO3
@anandpanchal63903 жыл бұрын
@@AnifG million of thanks sir🙏🙏
@dannysoni35187 ай бұрын
Does we need surface activator for gold plating on silver ... if yes tjen how can i make that
@alexandrerodrigues35312 жыл бұрын
Parabéns! Belo trabalho 🙏
@sonuverma27968 ай бұрын
How much volt and amp did u use for gold and rose gold plating
@billmusik9794 Жыл бұрын
can you use sodium Cynide ?
@DarveshKhan-j5d3 ай бұрын
Can i used 14k or 10k gold instead of 24k gold to make solution will it still work?
@BALITEKNIK0708093 жыл бұрын
Wow mantap tutorialnya, sukses buat channelnya
@AnifG3 жыл бұрын
Terimakasih om.. sukses juga buat anda 😊🙏
@MegaUsman423 жыл бұрын
Can you please tell, how much time per mg is required. Or how much time is sufficient to electroplate jewellery
@AndreiMorosan-km8ft8 ай бұрын
30 seconds
@Fashion.jpeg_2 жыл бұрын
Can this solution be used on 3d printed items? Do I need to spray anything on the 3d printed item first if so?
@hengkifernando40633 жыл бұрын
Mksh banyak ilmunya bg,itu kalau pakai air sepuh yg hambar buat campuran rose goldny boleh gk bg,trus klo hambarnya air rose gold itu di celupin warna jd apa bg
@hengkifernando40633 жыл бұрын
Mohon petunjuknya bg
@AnifG3 жыл бұрын
Air sepuh hambar itu gimana bang? Itu saya pakai air aquabides bang dicampur potas sama CuSo4..nanti pas mau pakai dikasi air emas dikit perbandingan (1:3)
@hengkifernando40633 жыл бұрын
@@AnifG mksh banyak bg🙏,mksudnya air emas bekas yg udh di celupin pengganti air emasny bisa bg?
@AnifG3 жыл бұрын
Oh iya bisa bang.. sy juga kadang pakai air emas bekas bang
@hengkifernando40633 жыл бұрын
@@AnifG maaf bg agak banyak tanya🙏🙏,tp hasilnya bagusan mana bg ya,dan bedanya apa bg
@techsvayrieng32802 жыл бұрын
Good brother,thank you. Have Other solution for make it bright or not?
@nishthagoel9285Ай бұрын
How do you determine the gold plating thickness?
@takishidz79616 ай бұрын
Does it need a precise voltage amont to use and does it have any impacte on the final result
@georgejosh18733 жыл бұрын
Bang itu air merahnya kalo ga dicampur sama yang emas bisa buat dasaran sepuh ga? Biar merah dulu baru disepuh emas gitu?
@sliceofbrain_2 жыл бұрын
Thankx for sharing your knowledge. May I know what is name of the electric machine you are using. And where can I buy it?
@sudendiyali19832 жыл бұрын
What type of water is this
@QUESTIONEVERYTHING.. Жыл бұрын
Distilled water
@dariovelasco73363 жыл бұрын
Como preparas tu solución para.blanquear tus piezas
@dariovelasco73363 жыл бұрын
Eso no contesta mi duda
@isawalter34653 жыл бұрын
que quieres decir con blanquear?
@deskmat987410 ай бұрын
Good to know I'm not the only one who writes electroplating with a k sometimes just because I felt like it
@bernardkorley6946 Жыл бұрын
So how long will such a playing last normally before you would have to plate it again
@harishrajamani49223 жыл бұрын
How to make cyanide free gold polishing Solution?
@oemorvillar97193 жыл бұрын
Any other name for CUSO? THANKS
@AnifG3 жыл бұрын
Chopper sulfate sir..you can get it on eBay or Amazon 🙏
@kushalmaulloo7622 жыл бұрын
Hi, i used the same process for 24k plating, but 1/2 quantity. But my jewelleries turned black and dull.. What did i do wrong please?
@wahyukuncorojati662 жыл бұрын
Terlalu lama ketika proses pewarnaan di dalam airnya. Menjadikan barang kusam. Cara untuk memulihkannya kembali dengan cara di poleshing. Dan di proses kembali.
@Avci__3 жыл бұрын
Can I not add cuso4?
@jacquesomersavard72572 жыл бұрын
I have lot of electronic gold part is it possible to use it in this process
@hyperhidrosissupport9186 Жыл бұрын
can i use potassium ferrocyanide instead of cyanide ?
@sudhar8898 ай бұрын
Hello sir is hcl and nitric acid concentrate on diluted? Please tell 😢
@nitin.m9033 жыл бұрын
Can we use potassium ferro cyanide also
@otavio27112 жыл бұрын
No.
@fatimaayub30612 жыл бұрын
Is this colour life time guarantee?
@LryuzakiLN11 ай бұрын
Lol, nothing last forever 😂 it's only for few months.
@rayaraya6720 Жыл бұрын
Potasium pakai potas apa ya mas agar air sepuhan tidak cepat berubah keruh
@isawalter34653 жыл бұрын
Hello Anif, could you PLEASE show us, how to get the gold out again of the solution, like somones asked already? That would be so great!
@AnifG3 жыл бұрын
Ok... Next time I will make a video
@karangandhi52163 жыл бұрын
Plz make it sir
@isawalter34653 жыл бұрын
@@AnifG Oh wonderful!
@sachinlohar11063 жыл бұрын
@@AnifG sir isme kitna kam niklta hai
@Anil80597soni3 жыл бұрын
Love from india
@AnifG3 жыл бұрын
Thank you so much 😊🙏
@MrMo7emad3 жыл бұрын
sir i want to ask you for 1 gr gold how many gr i can plat the silver
@AnifG3 жыл бұрын
For 1 gram of gold solution can be used for plating about 1.5 kg of silver or it can be for 2 kg of gold 🙏
@isawalter34653 жыл бұрын
@@AnifG can you express that in cm? thank you so much!