Hello.. Do you know how to run the chronocoulometry and calculate the surface area of an electrode ?
@058funbites4 ай бұрын
please can you explain IR compensation?
@udaykumarahuday1926 Жыл бұрын
How to prepare glassy electrode and provide basic information about electrolyte solution
@djexperimentsession4817 Жыл бұрын
Make con. Solution of your material in volatile solution and drop cast it on glassy carbon electrode And electrolyte solution should be made up of .5 M KOH or Na2SO4
@dr.shahidramay67287 ай бұрын
Why your EIS graph is not semicircle, it is showing high resistive but in my case no material is showing semicircle, please tell me the further conditions to set for Ch instruments?