In this video you can learn how to recover gold without using ready made nitric acid. KNO3, H2SO4, HCl, Gold Precipitation using Iron sulfate. Watch our video and if this helpful then don't for get to gives me a thumps up.
Пікірлер: 65
@shineyrocks3906 ай бұрын
These are the things that those big gold miner channels do not show. I appreciate you sharing your knowledge, thank you.
@PoorMiners3216 ай бұрын
Thank you
@willamsrodriguez88646 ай бұрын
Un saludo desde Venezuela reciba muchas bendiciones por sus enseñanzas en cada video que usted sube una duda el estaño de las soldadura dónde se queda gracias
@PoorMiners3216 ай бұрын
gracias hermano, si usas este método, si hay soldadura, se disolverá en ácido clorhídrico y permanecerá allí en la solución, luego capturará las láminas de oro y luego procederá a nuestro proceso.
@nikolasvasiliou2806 ай бұрын
Good evening, thank you very much, I had a problem with nitric acid and you gave me a very nice solution !!
@PoorMiners3216 ай бұрын
Welcome brother and thank you very much..
@julianalcorso57036 ай бұрын
Good work. Love your channel!
@PoorMiners3216 ай бұрын
Thank you..
@EmmaBSanta886 ай бұрын
It looks like a awesome procedure amazing
@PoorMiners3216 ай бұрын
Thanks
@ivanchrismarquez99912 ай бұрын
ang galing talaga nito, salamat sa mga tip and instructions master poor miner
@PoorMiners3212 ай бұрын
Thanks bro
@mariakoamigo73026 ай бұрын
Fantástico. Es más oro del que me esperaba
@PoorMiners3216 ай бұрын
Thanks.
@mariakoamigo73026 ай бұрын
Hola. En el minuto 4:50 aprox muestras las láminas de oro en el filtro y los residuos de las T-CON pero quedan aún láminas de oro en ese material. Recomiendo usar disolvente con el material antes de empezar, así eliminas adhesivo de los Flex y se suelta todo sin perder oro. Así lo hago yo y en 7 días está el material super limpio. El oro no se puede perder Muchísimas gracias por el vídeo. Suerte en la vida
@PoorMiners3216 ай бұрын
Thank you bro
@franguimfrangoso1046 ай бұрын
Parabéns poor Miner 💎🇧🇷
@PoorMiners3216 ай бұрын
Thank you..
@Elites-asthetic6 ай бұрын
Hello love the videos I have collected ram gold fingers only a total of 1kg Can I ask is this worth doing or collect more ?
@PoorMiners3216 ай бұрын
thank you brother, you can recover that is more than 1grams of gold it depends the quality of gold plating but if you want more, add more..
@donmmmatos2 ай бұрын
GENIAL! OBRIGADO PELAS DICAS.
@PoorMiners3212 ай бұрын
Thanks
@danielflinn35716 ай бұрын
Thanks from Australia
@PoorMiners3216 ай бұрын
Thank you..
@ignacio30486 ай бұрын
Thanks for sharing 😊
@PoorMiners3216 ай бұрын
Thanks for watching!
@angelooldman72016 ай бұрын
you are the best my friend ,thank you
@PoorMiners3216 ай бұрын
Thank you brother
@clovisalves12456 ай бұрын
Adoro seus vídeos, vejo com muita atenção p aprender, thank You Brasil
@PoorMiners3216 ай бұрын
Thank you very much.. I make portuguese subtitle for you my friend, all you need is to turn on cc above the video to see portuguese subtitle
@clovisalves12455 ай бұрын
Muito bom, Obrigado
@clovisalves12455 ай бұрын
Muito bom, Parabéns Brasil.
@PoorMiners3215 ай бұрын
Thank you
@miltondamiao65406 ай бұрын
Vídeo top,parabéns.
@PoorMiners3216 ай бұрын
Thank you..
@hossamslime93546 ай бұрын
Nice video We can used sodium nitrate indeed of potassium nitrate
@PoorMiners3216 ай бұрын
Yes you can, yes, it's possible as long as it's nitrate salt
@clovisalves12455 ай бұрын
Como está vc td bem? Não encontro o nitrato de sal, posso usar o que? Deus te abençoe!!
@PoorMiners3215 ай бұрын
Use chlorine its work better also
@bazonis1gp6 ай бұрын
👍👍❤
@PoorMiners3216 ай бұрын
Thanks
@bharatkhanna81486 ай бұрын
who is best food grade smb Or lab grade smb
@PoorMiners3216 ай бұрын
Thats the same effect brother, technical grade or lab grade expensive than food grade which is cheaper and the same effect for gold precipitation, if you use Iron sulfate thats much cheaper than smb and work also better
@harryniedecken53216 ай бұрын
Thank you for the great videos. Please be careful with your hands, as those goves are not acid resistant.
@PoorMiners3216 ай бұрын
Thanks, yeah thats why i always prepare tub full of water beside my jod if incase, but this latex gloves is similar to butyl gloves which is highly acid resistant, but as I said, always prepare water beside your work, and always present of mind that your working with acid.
@CrazyGoat-iy1qi28 күн бұрын
Cuánto se recobra en dinero, con referencia a la inversión, pues de caso contrario es preferible desechar esos componentes electrónicos en las áreas designadas por la ciudad, para evitar la contaminación ambiental. 😊😊😊😊
@PoorMiners32128 күн бұрын
Eso fue 4.534 pesos filipinos, hermano 79,54 USD, costo total 5 USD incluidos los productos químicos, nuestra ganancia 74,54 USD.
@clovisalves12455 ай бұрын
Rota 66 na sua terra, ou não?Abraço!!
@mustaphamus77176 ай бұрын
اللهم صل وسلم وزد وبارك على نبينا محمد صلى الله عليه وسلم تسليما كثيرا
@PoorMiners3216 ай бұрын
Thank you very much..
@ozcanozcelik66256 ай бұрын
Kolay gelsin selamlar
@PoorMiners3216 ай бұрын
Thank you..
@akgoldbear76696 ай бұрын
2:24 The highest concentration of hydrochloric acid is 36% at a density of 1.18 g/cm3. Your hydrochloric acid is 35%! Jesus Christ, where did you get such powerful acid?! 🙂 I want too.
@PoorMiners3216 ай бұрын
Yes this is very good hydrochloric acid in our country there are company making this concentration for swimming pool, this acid too much fumes when you open the cap.
@GemsPh5 ай бұрын
Sir tanong san poh maka bili ng nitric acid ...sana masagot salamat.
@PoorMiners3215 ай бұрын
Sa cebu marami daw doon
@GemsPh5 ай бұрын
@@PoorMiners321 sir anong maganda at effective na pag neutralize ng nitric acid sana masagot
@PoorMiners3215 ай бұрын
Sulfamic acid bro, wag gumamit ng urea hindi nakaka neutralized ng nitric yun.
@roshangatrazz64455 ай бұрын
How to recover dissolved gold from sulphuric acid?
@PoorMiners3215 ай бұрын
If ever your gold dissolve in sulfuric acid, prepare distilled water into beaker five times the volume of sulfuric acid, boil the distilled water then pour slowly sulfuric acid to hot distilled water, the gold precipitate, add distilled water if needed, then capture the gold to filter paper then proceed to aqua regia.
@roshangatrazz64455 ай бұрын
Actually I work to make gold jewellery and some of the time when I clean thin jewellery by sulfuric acid by heating it to the high temperature and pour some potassium nitrate the gold gets loss. Does it happens to me only or technically possible can you explain? And how to recover it actually?
@roshangatrazz64455 ай бұрын
And our work it has contains 99.4% gold 4% silver and remaining is zinc percentage.
@PoorMiners3215 ай бұрын
Concentrated sulfuric acid can dissolve gold when heated in a high temperature specially mix a few amounts of nitric acid, and the nitric acid doesn't dissolve gold we know that. The possible happen here when sulfuric acid react to nitrate salt it produce nitric acid, because nitric acid isn't separated to sulfuric acid it dissolved your gold because of the present of sulfuric acid, for better result of your work you must separate sulfuric acid and nitric acid to avoid any complecations of your work, you can make 10% nitric acid thats really good for jewelry cleaning.
@ednasvariance9052Ай бұрын
I think you r a chemist pero ang daming step Pala . Alin ang mas maganda compared to burning w/ fire
@PoorMiners321Ай бұрын
Hindi ko kilala yung mga ganyang pamamaraan bro..pero marami pa po tayong paraan na mas madali pa.