Another great video. You just showed me why I struggle so much with several of those films like the one on the right
@Dad_at_505 ай бұрын
Just stared yesterday you guys sure make it look easy . Thank you for the videos
@LiquidConceptsUSA5 ай бұрын
Our pleasure!
@리페어맨 Жыл бұрын
Dear Brian, Thank you so much for letting me know your know-how.
@LiquidConceptsUSA Жыл бұрын
You are most welcome!
@andrewlloyd4702 Жыл бұрын
Thanks for the videos.
@LiquidConceptsUSA Жыл бұрын
You're welcome!
@Blimpus Жыл бұрын
This was extremely helpful, Thank you for this one
@LiquidConceptsUSA Жыл бұрын
Glad it was helpful!
@hobbyprison Жыл бұрын
Thanks for the vid. Helpful! Would have liked to see how it dipped with a longer soak time.
@brandonemmanuel4994 Жыл бұрын
What a legend
@LiquidConceptsUSA Жыл бұрын
Thanks
@henrysara7716 Жыл бұрын
Great video, thy.
@LiquidConceptsUSA Жыл бұрын
Thanks !!
@STVenom225 Жыл бұрын
Would be good if you made a film sit time on a chart for before you activate and after.
@delonv9518 Жыл бұрын
How do u take spray chrome off plastic parts?? Do u have any suggestions?
@mohamadtivolii Жыл бұрын
thanks for the video but i would have loved to see how it dipped with the right amount of time
@KarterMorey24 Жыл бұрын
How much film would I need to dip a shotgun I am looking to dip one but I don’t know how much film to buy
@LiquidConceptsUSA Жыл бұрын
We sell film in meters. 1Meter is 39.37 inches. We offer 1Meter wide film & 50cm wide film. Hope that helps.
@PaulCapello Жыл бұрын
i havent seen any "soak time" reccomendations for films on your website.
@LiquidConceptsUSA Жыл бұрын
All films we recommend a 60 second soak time. There are a very few that require additional soak time and those are all noted in those films product description.
@jesussantibanez6711 Жыл бұрын
👍🏼👍🏼👍🏼👍🏼
@LiquidConceptsUSA Жыл бұрын
Thanks !!
@MichaelSlackta Жыл бұрын
Your in house film with the plastic backing does not even begin to break down after 60 seconds as per your included instructions.
@LiquidConceptsUSA Жыл бұрын
Hi Michael can you shoot me an email or give me a call to discuss. This does not sound correct but I need to know more information to diagnose. Also did you watch the video with the instructions to be sure you were laying the right side on the water and using it properly?
@andrewlloyd4702 Жыл бұрын
Can you please do a video, showing preparation, base coat choice etc, is there any list for base coats that go with the films?
@LiquidConceptsUSA Жыл бұрын
Most all base coats are listed on our website for each film. We do have a few separate prepping videos as well as how base colors can affect your film on our channel if you want to give it a look.
@craigalex8860 Жыл бұрын
I’m new to hydro dipping and wanted clarification on soaking in warm or cold water what do you recommend?
@LiquidConceptsUSA Жыл бұрын
We recommend 80-90 degrees for your tank water temperature