After watching this video you will be able to write a welding procedure specification (WPS) on your own.
Пікірлер: 130
@jamienoh67264 жыл бұрын
I had WPS class before for a week and paid 200USD. But this 30min. lecture is much better. thanks sir. from Korea
@WeldingandNDT4 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@manojr22825 жыл бұрын
the most awaited videos sir.. even bosses or seniors what I had seen are not willing to share their knowledge because of their ego and selfishness you are doing a great thing sir thank you so much👍👍👍
@WeldingandNDT5 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com
@anewyoutuber3 жыл бұрын
It’s not an Ego. But they are just afraid if you are going to be better than them. Its more political than selfishness. Anyway.. happy learning..
@pvenkatesh77303 жыл бұрын
Right
@jaisudhikshs75032 жыл бұрын
@@WeldingandNDT sir what is the P number for mild steel A5.1
@AhmedSaeed-lw5gb Жыл бұрын
all i can say is beautiful, no gibberish here or there stuff. direct to point and with examples and precise info.
@ansari44173 жыл бұрын
I am very happy to see this video it's very helpful for us
@WeldingandNDT3 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@evolati124 жыл бұрын
This right here is one of the main things that makes KZbin great: good, informative, free education. Sometimes a little difficult to understand but hey you can’t bitch when it’s free and the guy knows what he’s talking about!
@WeldingandNDT4 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@evolati124 жыл бұрын
Welding and NDT Will do. Appreciate it.
@hameedahmed7484 жыл бұрын
great video,i learned a lot from your comments and professional wording
@WeldingandNDT4 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@XTREND_KSA4 жыл бұрын
Sir, you are a life saver!
@WeldingandNDT4 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@rubangrg5 жыл бұрын
Sir You are great to share your knowledge,
@WeldingandNDT5 жыл бұрын
Thanks. Please visit my website weldingandndt.com
@ahmadmohammed62252 жыл бұрын
Than you very much sir .. I have learned a lot from this vedio ..
@WeldingandNDT Жыл бұрын
Thank you. Please join my channel. Joining Link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@titofernandezl3 жыл бұрын
Good video No lag Points explained Easily understandable full star rating for this
@WeldingandNDT3 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@chidiiwegbula74244 жыл бұрын
Thank you for sharing your immense knowledge..well done sir
@WeldingandNDT4 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@karthikeyanvenkatraman47153 жыл бұрын
Excellent presentation sir please show each table from the standard and please fill all tables with an example in the next video. That will be really helpful
@WeldingandNDT2 жыл бұрын
Thank you. Please join my channel to support me. Joining Link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@mahasindhudey92642 жыл бұрын
Very good and help full. Thank you
@WeldingandNDT2 жыл бұрын
Thank you. Please use the below link to join my channel: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@farhaniftikhar23794 жыл бұрын
You have done a great job. Thanks for the lesson.
@WeldingandNDT4 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@thirupathieppapula50263 жыл бұрын
Great and your teaching and it help me alot thank you
@WeldingandNDT3 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@Twenty_four_into_seven_vlogs5 ай бұрын
Productive videos thank you sir
@WeldingandNDT4 ай бұрын
Thank you. Please join my channel to support my initiative. Joining link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@anilkumarsahoo67853 жыл бұрын
Very nicely explained.
@WeldingandNDT3 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@muhamedsafvan75242 жыл бұрын
Great job well done sir👍👍
@WeldingandNDT2 жыл бұрын
Thank you. Please join my channel to support my initiative. Joining Link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@KrishnaDas-cq3kh Жыл бұрын
Very excellent Sir. Thanks a lot
@WeldingandNDT Жыл бұрын
Thank you. Please join my channel to support my initiative. Joining link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@mohamedabdou33843 жыл бұрын
Great Effort From You, Thanks So Much
@WeldingandNDT3 жыл бұрын
Thank you. Please join my channel to watch all the videos. Joining link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@jyothisthomas27055 жыл бұрын
Thanks for your efforts sir
@amalababu918 ай бұрын
Really Good content ✨🤝✨ Thanks 👍
@GyanPrakash-po7bn4 жыл бұрын
excellent presentation and with all tech details ,regards
@WeldingandNDT4 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@paramasivamsubbiah37424 жыл бұрын
nice very clear and you made it easy sir
@ismaeljamin79874 ай бұрын
Very good explanation
@WeldingandNDT3 ай бұрын
Thank you. Please join my channel to support my initiative. Joining Link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@mohamedferoz29132 жыл бұрын
Good video content
@WeldingandNDT2 жыл бұрын
Thank you. Please join my channel to support me. Joining link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@weldingtechnologytechnical48203 жыл бұрын
Very nice Vedeo
@WeldingandNDT3 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@fvsood5 жыл бұрын
Great video !
@WeldingandNDT5 жыл бұрын
Thanks. Please visit my website weldingandndt.com
@SaifKhan-hg7so2 ай бұрын
Great 🎉🎉🎉
@WeldingandNDTАй бұрын
Thank you. Please join my channel to support my initiative. Joining link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@mppramosh89405 жыл бұрын
Great work sir thank you very much sir
@WeldingandNDT5 жыл бұрын
Thanks. Please visit my website weldingandndt.com
@sandeepchaubey55675 жыл бұрын
Sir please explain about backing And how to find A No for different welding consumables
@aravindjothimurugan22013 жыл бұрын
Nice video and good work. 👏👏👏👏 You explanation was very nice and clear-cut. Keep going and put more videos , you will be more fame in near future. Looking forward to your next video 👍
@WeldingandNDT2 жыл бұрын
Thank you. Please join my channel to watch all the videos. Joining Link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@srinivassai46964 жыл бұрын
Thanks for your explanation and it's helpful 👍😀😁
@WeldingandNDT4 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@mr34chanti3 жыл бұрын
U should write all the points.. codes is not required keep it up sir. Please do another video with all overview of points
@raufbasra21165 жыл бұрын
Sir please make video on material test certificate
@simonwong61722 жыл бұрын
Very informative, thank you.
@WeldingandNDT2 жыл бұрын
Thank you
@allinonebyakk78782 жыл бұрын
Awesome 💥🙏
@WeldingandNDT2 жыл бұрын
Thank you. Please join my channel to watch all the videos. Joining Link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@savanraval14893 жыл бұрын
1-2 mm should be there for root face instead of 1-2 m; overall video is so helpful Keep uploading more videos
@noblepayyappilly7913 Жыл бұрын
Hi can I ask one doubt
@rahulprasannan55533 жыл бұрын
Super class
@rudycesneros51224 жыл бұрын
Thank you very much for knowledge sharing.
@WeldingandNDT4 жыл бұрын
Thank you. Please visit my website for notes, videos and other important informations www.weldingandndt.com/
@kajjumaideen85617 ай бұрын
Thank you 🎉
@ramu0412 жыл бұрын
Sir,for weld overlay what is thickness range ( pqr and wqt)if deposited weld metal is 2mm in 1inch plate .And the what should be the total width to be deposited in pqr and wqt
@abderrahmanebenabdallah6725 жыл бұрын
Great work thank you sir
@WeldingandNDT5 жыл бұрын
Thanks. Please visit my website weldingandndt.com
@raeesshaikh66784 жыл бұрын
Great knowledge but In PWHT T for thickness of Material not you mentioned it (Temperature 22:59 to 23:13 please refer it )
@tanveerahmed65254 жыл бұрын
Dear Sir , Your way of presentation is Awesome And Thanks a lot for Sharing your valuable knowledge Can you plz make a video on Demand of Job market based on coating inspector Courses like SSPC/B-GAS/NACE CIP LEVEL-1 & 2 ..Which will be better Among those
@WeldingandNDT4 жыл бұрын
Thanks a lot. Please visit my website www.weldingandndt.com/
@mani4r5 жыл бұрын
Will you please start teaching important chapter of ASME code. If you are planning so please reply.
@liyakatsherasia83775 жыл бұрын
request to make video on how to review MTC
@naouelsalematia93253 жыл бұрын
Thank you so much
@WeldingandNDT2 жыл бұрын
Thank you. If you want to financially support me, Please join my channel. Joining Link: kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@mehmetatar4435 жыл бұрын
Good video and giving many details, I think, if you have time you should get one more time this video to clear explanation, thank you
@WeldingandNDT2 жыл бұрын
Thank you. Please join my channel to support my initiative. Joining Link:kzbin.info/door/H7nXSievFlbRKzKzEySbkwjoin
@hamzarasheed12322 жыл бұрын
@26:26 For specifications of shielding gas, the correct name is SFA-5.32 in ASME Section II Part C (2019)
@begobi0075 жыл бұрын
How to fix heat input limits(max)? Is there any reference code for that? I know formula.
@johndavisdavis67334 жыл бұрын
Sir please share formula, it will help for others
@shortvideos55135 жыл бұрын
Please make video on Bgas (coating Inspector)
@musondampandashulu64705 жыл бұрын
Hey Nandeep, just watched WPS writing video in English. Very educative. Thanks lots. Would you also touch PQR`s, like when you need a new PQR?
@WeldingandNDT5 жыл бұрын
Thank you. I will upload videos on PQR too. Please visit my website www.weldingandndt.com
@nidhishknk5013 жыл бұрын
Thank you
@WeldingandNDT3 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@noblepayyappilly7913 Жыл бұрын
If we preparing wps for 25 mm plate process gtaw+smaw how we get the deposit weld metal for gtaw and smaw
@tapaspanda503 жыл бұрын
Sir make a video on Piping Execution Engineer related questions and answers for interview .
@praveenav73302 жыл бұрын
Sir, please explain how do I write , specification type and grade of material in WPS.
@rao416able4 жыл бұрын
Please make a video on the use of UCS 66 CURVE for charpy test exemption criteria
@afzalsaifi49462 жыл бұрын
What is SFA specification of GTAW welding for carbon steel filler wire? SFA 5.9 or 5.18
@praveenav73302 жыл бұрын
Hi sir, please let me know how to write "specification type and grade " in WPS. as per Qw.422 Specification SA (asme) , but all WPS having ASTM specification. How can I know ASTM specification table ? And one more question, eg. For p number 1 material there are lot of material specification in Qw. 422 how can I select which material specification need to write in WPS table ? Sir please answer my question.
@abdulsamee12234 жыл бұрын
How we are selecting F & A number For F number we can select 7018, 6010, 7010 etc any one we can select or can we refer any table for F Number for and particular material for this filler ???
@WeldingandNDT4 жыл бұрын
For F no and A no for a filler material there is table in ASME sec IX. Thank You. Please visit my website www.weldingandndt.com/
@begobi0075 жыл бұрын
Why A number mandatory and why there is no such a thing (A No) for dissimilar materials is not a mandatory?
@jithmonnp81285 жыл бұрын
Hi can you upload a video regarding RTFI
@mohammedkadhim94834 жыл бұрын
hi sir i have Q is that applied on storage tank or only for piping?
@ashishghadiya95785 жыл бұрын
Sir, I enjoy and learn welding concept in detail from your videos.Thank you very much for knowledge sharing. If you have any questions list(With answer if possible) regarding welding and pressure vessel fabrication which may help in interview,please share with us or drop me mail if possible.
@WeldingandNDT5 жыл бұрын
Thanks. Please visit my website weldingandndt.com
@priyankavincent18804 жыл бұрын
sir which ASME section we can get the interpass temperature details?? kindly reply
@mutazmumin11 күн бұрын
What about pipe diameter?
@souravbohrays41894 жыл бұрын
try for clad and overlay wps that will be great
@WeldingandNDT4 жыл бұрын
Thank you. Please visit my website www.weldingandndt.com/
@muhammedsalih72844 жыл бұрын
For shielding gas, it is not SFA-5.3.2. It is SFA-5.32
@shahroohsmdw8424 жыл бұрын
Please do the video on ASME sec VIII
@himanshukatakiya63405 жыл бұрын
Unable to download it... Plz help
@MrPravean Жыл бұрын
Dear sir I am your you tube subscribe video is good useful tips I need help regarding clear explanation regarding ApI 1104 specially different type of welder qualifications can you make video about this
@sougatasen85373 жыл бұрын
Electrical characteristics in not clearly understood by me Sir.. please sir tell me how to write electrical characteristics...
@ramraj77015 жыл бұрын
Not both root face.one is root gap
@rubangrg4 жыл бұрын
Dear Sir, i have a confusion in wps, pqr and welder qualification.. My question is who is eligible to write and qualify the above. Or do we need CWI or any special welding inspector to write and qualify.. Need your valuable advice..
@sahebhussain85034 жыл бұрын
Contractor will give pwps.based on pwps tpi/client conduct eqt&PQT and send test coupon in lab for DT test.after meeting requirement result as per code & construction ,wps will qualify/approved