The process of manufacturing (forging) a blade from a rope. On the cutting edge, steel is W 110, zone hardening is 62 units.
my website: sites.google.com/site/damasks...
Frequently Asked Questions: The roller is long - but not a single stroke is missed on the steel. The billet is soaked in kerosene. This is necessary for good welding (forging) steel. I sprinkle flux (90% borax + 5% quartz sand + 5% charcoal powder) this is necessary for forging (forge) welding. The flux is alloyed with scale - the formed substance is sufficiently fluid and is easily displaced by deformation. In addition, the flux protects against oxygen and charcoal, carburizes the surface layer of metal - which lowers the welding temperature (if in brief). I do not answer the question of cost - write to the mail: sites.google.com/site/damasks...