why orthophosphoric acid on already etched porcelain surfuce !!!!
@drabyad24986 жыл бұрын
After hydrofluoric acid etching of the ceramic a layer of salts develops on the surface which acts as a barrier preventing good priming of the surface. Phosphoric acid is thought to remove these salts and dissolve them for a fresh surface. (However this is an arguable matter and some argue against its use)
@c_lent5 жыл бұрын
@@drabyad2498 the phosphate groups in the phosphoric acid fight to bind with the phosphate groups in the cement less adhesion to the crown/tooth interface. Not recommended anymore
@dr.sham1 Жыл бұрын
Can i use this silane in the attached photo from 3M 3M™ Silane Coupling Agent, 68300
@romerodentalseminars Жыл бұрын
Yes you can.
@elenzaable4 жыл бұрын
What container is used to carry the veneer when place in ultrasonic bath
@romerodentalseminars4 жыл бұрын
Elenza Jacob plastic container
@SmilesByDesignAdmin3 ай бұрын
is the cement light cure or dual cure?
@AHMEDSAlAH-qv3ss3 жыл бұрын
Are u washing silane with water??
@81od3 жыл бұрын
Logically No !
@AHMEDSAlAH-qv3ss3 жыл бұрын
@@81od dry by air only ?? then put adhesive bond or what the next step ??
@81od3 жыл бұрын
@@AHMEDSAlAH-qv3ss dry by air only then put your adhesive..with variolink you don t need to put adhesive in the veneer..you put it only in the tooth surface
@AHMEDSAlAH-qv3ss3 жыл бұрын
@@81od thank u Dr , all the the best to you❤👍
@81od3 жыл бұрын
@@AHMEDSAlAH-qv3ss not at all Dr Ahmed Saiah..you re welcome.!
@heartOFlino5 жыл бұрын
Thanks a lot for the video ❤️
@user-hd3hy4co1h3 жыл бұрын
What about applying bonding ,cement and veneers and cure it at the same time ,don’t you think it’s better?
@dr.davident3 жыл бұрын
Why?
@user-hd3hy4co1h3 жыл бұрын
@@dr.davident actually I need to know if it’s ok or we will face problems later ,there is a theory says do one step curing (bonding ,cement and veneers) so we will not lose the fitting
@sherafati9 ай бұрын
@@user-hd3hy4co1h You can not ensure that you get a proper hybrid layer if you co-cure. You need to cure the bonding agent on tooth surface separately to make sure you get a good hybrid layer. As for sitting issues, you need to completely air thin the bonding agent.
@revsen64054 жыл бұрын
Which resin cement is recommended
@romerodentalseminars4 жыл бұрын
LEGANDARY GAMING NX3 Kavo Kerr
@caner18103 жыл бұрын
Wished to see every step under high magnification
@يوسفمازنيوسف-ز7و4 жыл бұрын
Although the ceramic material is brittle material ,but we can use it in less than 1mm for facial and occlusal veneer ..why??
@emyfekry33444 жыл бұрын
Porcelain is brittle like natural tooth but porcelain is so hard to withstand chips and cracking although wrong or heavy frequent compact forces could cause fracture by the way. So it's indicated as veeners or full crowns just for anterior teeth where no heavy forces might be applied on likewise posterior teeth
@nutellaluis6833 жыл бұрын
@@emyfekry3344 can it br used for 2 or more units bridge for the anteriors or just for individual crown?
@louisbarros97576 жыл бұрын
Quick question Mario, what do you think about curing the bond prior to cement application? Does it make any difference? I see you cure everything all at once, does this give better results? Thanks for sharing!
@romerodentalseminars6 жыл бұрын
Louis Barros I cure the adhesive layer prior to bonding the restoration. For me it is critical to have a fully polimerized hybrid layer and curing all at once can create some problems if it does not reach the adhesive layer with the needed energy.
@puneetsekhon34363 жыл бұрын
@@romerodentalseminars did you cure the bond on the intaglio surface of the veneer before applying the cement?
@romerodentalseminars3 жыл бұрын
@@puneetsekhon3436 No, you should not cure.
@puneetsekhon34363 жыл бұрын
@@romerodentalseminars thanks for the prompt reply, appreciate it. What is the reason behind not curing it before the cement?
@romerodentalseminars3 жыл бұрын
@@puneetsekhon3436 the use on bonding agent in the intaglio surface is only to improve “wetability” of the resin cement to the silanated glass surface.
@dr.davident6 жыл бұрын
Ultrasonic not ultrasound ! and thanks for the amazing video :)
@romerodentalseminars6 жыл бұрын
Thanks for catching the typo. We will correct it.
@kamhuong60954 жыл бұрын
What's the difference between those words?
@salilfloyd48043 жыл бұрын
Can we use luting GIC ??
@LoLFilmStudios Жыл бұрын
Absolutely not.
@MrLukeanthony6 жыл бұрын
What a dreadful shade match
@LoLFilmStudios Жыл бұрын
This video is supposed to show the process of cementation, not color matching. You commented negatively in only way you knew how. It says three things: You don't know much. You're craving negativity. Your comment is irrelevant.