It would be interesting to see a before and after shot of these parts to see how the surface condition changes due to corrosion.
@tvviewer45009 ай бұрын
What did you just look at?
@metallurgysoup9 ай бұрын
@@tvviewer4500touché. I could have been more specific. The corrosion product obscures the metal surfaces at the end of the video. Cleaning the corrosion products (rust, oxides, etc.) off the parts would allow for a clearer comparison of the effect of corrosion on the base metals (material loss, pitting, etc.).
@Itrieditathome88910 ай бұрын
If you want to know the damaging effects of galvanic corrosion all you need to do is try to change a wheel bearing on a ford explorer with aluminum knuckles.
@Shane_at_SteelImage10 ай бұрын
Haha.... maybe I should not be laughing...
@tvviewer45009 ай бұрын
@@Shane_at_SteelImageWhy, ford's design team and dealership garages are laughing
@westonlee97785 ай бұрын
Do you know if a brass fitting screwed into an aluminum gas tank would create corrosion? Thank you for you video