6G Inconel, max TIG Welding Procedure F34, F4X ! Welder performance qualification with tig filler wire ER NiCrMo-3, Inconel refers to a group of specific nickel-chromium alloys used in different welding processes. Inconel is most commonly used in techniques that require a high heat tolerance. Welding Inconel can be rather difficult because the welds that are created have a tendency to crack.
6G position requires one pipe to be positioned at a 45-degree angle. This weld is considered the most challenging type of weld to perform because it requires welds that are made in all positions. The root process is a weave over a filler rod. Hot pass by getting the tow of the pool to the walls, protecting root.
#6G #tig #extremetig
None of these videos are recorded in a fancy shop surrounded by sponsorship banners!
All of my videos are recorded at working sites in various locations and in different welding positions.
90% of my welding projects in videos are x-rayed, and if you like to see hands-on projects, welcome!
If you liked this video please give it a thumbs up, share it, subscribe, and click the bell.
It doesn’t cost you anything but it massively helps my KZbin channel. Thank you.
Support this channel with 🔔 Subscribe and 👍 Like!
/ x3mtig